Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.530 - 1.30 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
0.993 - 2.44 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne |
|||
Izod Impact, Notched | 0.0981 - 1.30 J/cm | 0.184 - 2.44 ft-lb/in | Average value: 0.294 J/cm Grade Count:58 |
Overview of materials for Polystyrene, Heat Resistant Grade This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.260 - 1.30 J/cm @Temperature -30.0 - -30.0 °C |
0.487 - 2.44 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.758 J/cm Grade Count:6 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.600 - 1.30 J/cm @Temperature -30.0 - 0.000 °C |
1.12 - 2.44 ft-lb/in @Temperature -22.0 - 32.0 °F |
Average value: 0.875 J/cm Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.600 - 1.30 J/cm @Thickness 3.17 - 3.17 mm |
1.12 - 2.44 ft-lb/in @Thickness 0.125 - 0.125 in |
Average value: 0.875 J/cm Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Izod Impact, Notched | 0.350 - 1.30 J/cm | 0.656 - 2.44 ft-lb/in | Average value: 0.771 J/cm Grade Count:23 |
Overview of materials for Polyarylamide, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyarylamide, Glass Fiber Filled". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.800 - 1.30 J/cm | 1.50 - 2.44 ft-lb/in | |
Solvay Specialty Polymers Hylar® MP10 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Izod Impact, Notched | 0.250 - 1.30 J/cm | 0.468 - 2.44 ft-lb/in | Average value: 0.478 J/cm Grade Count:50 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Notched | 0.800 - 1.30 J/cm @Thickness 6.35 mm |
1.50 - 2.44 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT3030 30% Glass Fiber Enforced PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.700 - 1.30 J/cm @Thickness 6.35 mm |
1.31 - 2.44 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT4830 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.700 - 1.30 J/cm @Thickness 6.35 mm |
1.31 - 2.44 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT4130 Fire Retardant & 30% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.800 - 1.30 J/cm | 1.50 - 2.44 ft-lb/in | |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Izod Impact, Notched | 1.30 - 1.30 J/cm @Temperature -40.0 - -40.0 °C |
2.44 - 2.44 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.30 J/cm Grade Count:2 |
Overview of materials for Polypropylene, Glass Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass Reinforced, Impact Modified". Each property range of values reported is minimum and.. |
|||
Izod Impact, Notched | 0.400 - 1.30 J/cm @Temperature -28.9 - -20.0 °C |
0.749 - 2.44 ft-lb/in @Temperature -20.0 - -4.00 °F |
Average value: 0.854 J/cm Grade Count:5 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Izod Impact, Notched | 0.160 - 1.30 J/cm | 0.300 - 2.44 ft-lb/in | Average value: 0.306 J/cm Grade Count:125 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Notched | 1.10 - 1.30 J/cm @Temperature -20.0 - 0.000 °C |
2.06 - 2.44 ft-lb/in @Temperature -4.00 - 32.0 °F |
Average value: 1.20 J/cm Grade Count:1 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |