Polymer Property : Izod Impact, Notched = 1.31 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.380 - 0.700 J/cm
0.712 - 1.31 ft-lb/in
Average value: 0.565 J/cm Grade Count:4
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep..
Izod Impact, Notched 0.280 - 0.700 J/cm

@Temperature -40.0 - -20.0 °C
0.525 - 1.31 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.321 J/cm Grade Count:4
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.500 - 0.700 J/cm
0.937 - 1.31 ft-lb/in
ASTM D256
Loxim 821 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant
Information provided by Loxim Industries
Izod Impact, Notched 0.500 - 0.700 J/cm
0.937 - 1.31 ft-lb/in
ASTM D256
Shuman 811 Black Polystyrene Medium Impact
Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer.
Izod Impact, Notched 0.500 - 0.700 J/cm
0.937 - 1.31 ft-lb/in
ASTM D256
Shuman 881 Grey Polystyrene Medium Impact
Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer.
Izod Impact, Notched 0.500 - 0.700 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
0.937 - 1.31 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256, ISO 180/4a
EPICHEM PA 6 GF 30 Polyamide 6, 30% Glass
Characteristics: medium viscosity, 30% glass fibre filled
Izod Impact, Notched 0.500 - 0.700 J/cm

@Thickness 6.35 mm
0.937 - 1.31 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT
Information provided by Dowell Trading Company Ltd.
Izod Impact, Notched 0.500 - 0.700 J/cm

@Thickness 6.35 mm
0.937 - 1.31 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
Izod Impact, Notched 0.600 - 0.700 J/cm
1.12 - 1.31 ft-lb/in
IS 13411-1992
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded
Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color..
Izod Impact, Notched 0.500 - 0.700 J/cm

@Thickness 6.35 mm
0.937 - 1.31 ft-lb/in

@Thickness 0.250 in
ASTM D256
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT
Information provided by Dowell Trading Company Ltd.
Izod Impact, Notched 0.600 - 0.700 J/cm

@Temperature -30.0 - 0.000 °C
1.12 - 1.31 ft-lb/in

@Temperature -22.0 - 32.0 °F
Average value: 0.692 J/cm Grade Count:1
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Izod Impact, Notched 0.600 - 0.700 J/cm

@Thickness 3.20 - 3.20 mm
1.12 - 1.31 ft-lb/in

@Thickness 0.126 - 0.126 in
Average value: 0.692 J/cm Grade Count:1
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..