| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
North Wood Plastics HDPE with 20% Wood Fiber
Data provided by North Wood Plastics, Inc.
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
SABIC M300054 High Density Polyethylene for Injection Molding
Product Description: M300054 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow..
|
|||
| Izod Impact, Notched | 0.280 - 1.80 J/cm | 0.525 - 3.37 ft-lb/in | Average value: 0.941 J/cm Grade Count:45 |
|
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
|
|||
| Izod Impact, Notched |
0.280
-
0.700
J/cm @Temperature -40.0 - -20.0 °C |
0.525
-
1.31
ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.321 J/cm Grade Count:4 |
|
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12
LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant.
|
|||
| Izod Impact, Notched |
0.280
J/cm @Temperature 23.0 °C |
0.525
ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
|
SABIC Innovative Plastics Valox® 175 PBT
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East)
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® 176 PBT
Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® 176HP PBT
Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® IQ3001 PBT (Europe-Africa-Middle East)
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
Sumitomo Bakelite Durez® 31735 Phenolic, Compression Grade
Durez 31735 is a special purpose phenolic molding compound developed for automotive and industrial pulleys. This material is designed to optimize pulley performance relating to belt life, dimension..
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics Valox® IQ3001 PBT
Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications.
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP M7002XXH PP
LNP* THERMOCOMP* M7002XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additives. Designed for touch surfaces in healthcare applications. Added features include:..
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
SABIC Innovative Plastics LNP THERMOCOMP RB004 PA 66
LNP* THERMOCOMP* RB004 is a compound based on Nylon 66 containing Glass Beads.
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
Goodfellow TPX® MX002O Polymethylpentene
This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi..
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D256 |
|
Cresset Powers Cress-Alon™ NF3020 2% Nano Clay Loaded, 3.0 r.v. Film Grade Nylon 6, 50% RH
Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib..
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM D-256 |
|
Axiall ProTherm® 4303 Rigid PVC, Extrusion
Georgia Gulf 4303 is a CPVC powder formulation designed for the processing of pipe products with an O.D. range of 1/2" to 8 inches requiring high heat deflection temperatures. Processing and stabil..
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM-D256 |
|
Braskem IB58 HDPE Injection Molding Polyethylene Copolymer
IB58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers good processability combined with good ..
|
|||
| Izod Impact, Notched | 0.280 - 0.420 J/cm | 0.525 - 0.787 ft-lb/in | IS 13411-1992 |
|
Amity Thermosets ATM 122 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane..
|
|||
| Izod Impact, Notched | 0.280 - 0.420 J/cm | 0.525 - 0.787 ft-lb/in | IS 13411-1992 |
|
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane..
|
|||
| Izod Impact, Notched |
0.280
J/cm @Thickness 3.20 mm |
0.525
ft-lb/in @Thickness 0.126 in |
ASTM D256 |
|
Beijing Chemical Industry KAIFA® HN301-G30 PA6 Resin
30% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Izod Impact, Notched | 0.280 J/cm | 0.525 ft-lb/in | ASTM-D256 |
|
Braskem IG58 HDPE Injection Molding Polyethylene Copolymer
IG58 is a high-density polyethylene, narrow molecular weight butene-1 copolymer produced by the solution process for injection molding applications. It offers high stiffness, impact strength and out..
|
|||
| Izod Impact, Notched | 0.280 - 0.370 J/cm | 0.525 - 0.693 ft-lb/in | IS 13411-1992 |
|
Amity Thermosets ATG 112 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic ..
|
|||
| Izod Impact, Notched |
0.280
J/cm @Thickness 3.20 mm |
0.525
ft-lb/in @Thickness 0.126 in |
ASTM D256 |
|
Beijing Chemical Industry KAIFA® 302-G0 PBT Resin
Flame retardant, low bleedingInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||