Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.430 - 0.600 J/cm @Temperature -40.0 - -20.0 °C |
0.806 - 1.12 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.554 J/cm Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Izod Impact, Notched | 0.500 - 0.600 J/cm | 0.937 - 1.12 ft-lb/in | Average value: 0.567 J/cm Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.400 - 0.600 J/cm @Temperature -40.0 - 0.000 °C |
0.749 - 1.12 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 0.475 J/cm Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.600 - 0.600 J/cm @Temperature 0.000 - 0.000 °C |
1.12 - 1.12 ft-lb/in @Temperature 32.0 - 32.0 °F |
Average value: 0.600 J/cm Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Notched | 0.550 - 0.600 J/cm | 1.03 - 1.12 ft-lb/in | ASTM D256 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Izod Impact, Notched | 0.500 - 0.600 J/cm | 0.937 - 1.12 ft-lb/in | ASTM D256 |
Loxim 315 01HB Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.400 - 0.600 J/cm | 0.749 - 1.12 ft-lb/in | ASTM D256 |
Loxim 820 01 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.500 - 0.600 J/cm | 0.937 - 1.12 ft-lb/in | ASTM D256 |
Loxim 830 12 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.400 - 0.600 J/cm | 0.749 - 1.12 ft-lb/in | ASTM D256 |
Loxim 831 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.400 - 0.600 J/cm | 0.749 - 1.12 ft-lb/in | ASTM D256 |
Loxim 841 02T HB Polypropylene Compound, 40% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.300 - 0.600 J/cm | 0.562 - 1.12 ft-lb/in | ASTM D256 |
Shuman 510 Black Polypropylene Homopolymer Excellent chemical resistance, excellent processabilityData provided by the manufacturer. |
|||
Izod Impact, Notched | 0.400 - 0.600 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.749 - 1.12 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM PA 66 Polyamide 66 |
|||
Izod Impact, Notched | 0.550 - 0.600 J/cm | 1.03 - 1.12 ft-lb/in | ASTM D256 |
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |
|||
Izod Impact, Notched | 0.500 - 0.600 J/cm @Thickness 6.35 mm |
0.937 - 1.12 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT1100L General Purpose PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.300 - 0.600 J/cm @Temperature -40.0 - -20.0 °C |
0.562 - 1.12 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.752 J/cm Grade Count:4 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |