Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shuman 510 Black Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Shuman
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shuman 510 Black Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Excellent chemical resistance, excellent processabilityData provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 5.0 - 8.9 g/10 min
5.0 - 8.9 g/10 min
ASTM D1238
9.0 - 12.9 g/10 min
9.0 - 12.9 g/10 min
13 - 16.9 g/10 min
13 - 16.9 g/10 min
17.0 - 22.0 g/10 min
17.0 - 22.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
ASTM D638
Izod Impact, Notched 0.300 - 0.600 J/cm
0.562 - 1.12 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °C
122 °F
ASTM D648
Vicat Softening Point 148 °C
298 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 188 - 216 °C
370 - 421 °F