Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.50 J/cm @Temperature 23.0 °C |
8.43 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Mytex Polymers AN16L(W)-D56 Polypropylene, Talc filled, Compounded, Elastomer, Impact modified Description: AN16L-D56 is a compounded talc filled elastomer modified polypropylene with good impact and excellent material flow properties.Key Applications: Automotive exteriorInformation provided .. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 23.0 °C |
8.43 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Mytex Polymers AS65KW-1ATM Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: Non-painted instrument panelInformation provided by Mytex P.. |
|||
Izod Impact, Notched | 4.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.43 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne OnForce™ LFT UR-50 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature -30.0 °C |
8.43 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature -30.0 °C |
8.43 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific) High impact PC+ABS material designed for local Pacific Automotive applications |
|||
Izod Impact, Notched | 4.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.43 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
PolyOne Geon™ CPVC EC900 Polyvinyl Chloride, Chlorinated (CPVC) The Geon EC900 CPVC is an extrusion compound for CTS Pipe applications where enhanced resistance at elevated temperatures is needed. It is listed under NSF Std 14 and 61. Geon EC900 demonstrates eas.. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature -50.0 °C |
8.43 ft-lb/in @Temperature -58.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature -50.0 °C |
8.43 ft-lb/in @Temperature -58.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors. |
|||
Izod Impact, Notched | 4.50 J/cm @Thickness 3.17 mm |
8.43 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Polimeri Europa SINKRAL B532 ABS, Very High Impact
(discontinued **) Very high impact; injection/extrusion grade.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
Gichem GIBLEND F70X3/VO ABS - Polycarbonate - PC/ABS Flame Retardant
(discontinued **) Blend PC-ABS self-extinguishing class V0 high fluidity. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Izod Impact, Notched | 4.50 - 6.4068 J/cm @Temperature -40.0 - 0.000 °C |
8.43 - 12.003 ft-lb/in @Temperature -40.0 - 32.0 °F |
Average value: 3.96 J/cm Grade Count:6 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Ixef® 3008 Polyarylamide (PARA)
(Unverified Data**) Ixef 3008 is a 30% carbon-fiber reinforced polyarylamide compound which exhibits extremely high strength and stiffness, good surface gloss, excellent creep resistance, and lower density than glass-f.. |
|||
Izod Impact, Notched | >= 4.50 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 8.43 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PC-S609 Toughened PC Features:Good mechanical propertiesSuper high impact strengthGood weather resistanceHigh glossGood processing propertiesStress cracking propertiesApplications:OA and IT partsAutomobile accessoriesEl.. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL CF-610 Electrically Conductive POM, 10% Carbon Fiber Filled, High Strength, Wear Resistant LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | edgewise; ASTM D256 |
Haysite H755 Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A new generation of IEEE Class F, 155ºC /165ºC NEMA GPO- 1 material. H755 is designed to bridge the gap between 130ºC Class B GPO-1 materials and Class H 180ºC grades. H755 has quickly g.. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature -30.0 °C |
8.43 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 0.000 °C |
8.43 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X2500UV PC+PET (Europe-Africa-Middle East) XENOY X2500UV is a medium viscosity, unfilled, elastomer modified PC/PET blend with excellent heat and impact performance. ISO1043-label: PC+PET-I. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
UBE UBESTA® 3020IX1 Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, impact modifiedInformation provided by UBE. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
Polyram RamLloy PBB106 PC/ABS Alloy, UV Stabilized UV stabilized PC/ABS alloy for injection molding applications.Information provided by Polyram. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 4.50 J/cm @Thickness 3.17 mm |
8.43 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika FUN-8000 Characteristics: High impact strength High chemical resistance Transparency as high as polycarbonateInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 23.0 °C |
8.43 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron A50B02 Nylon 66, Chemically Coupled 50% Long Fiber A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature -30.0 °C |
8.43 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers Tekaloy® G70A3 , Heat Resistance, Easy Molding PC/ABS Alloy Heat Resistance, Easy MoldingInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Izod Impact, Notched | 4.50 J/cm @Temperature 23.0 °C |
8.43 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron A50N02 Nylon 66, Chemically Coupled 50% Long Fiber A CHEMICALLY COUPLED 50% LONG FIBER GLASS REINFORCED NATURAL NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 4.50 J/cm | 8.43 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 3701 Information provided by A. Schulman. |