Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded, Flow; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L0313 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 600 A 44 Black 13 Polyamide 6 (Nylon 6) The Nymax® GF 600 Series of glass fiber-reinforced nylon 6 compounds have been specifically engineered for applications requiring high stiffness, tensile strength, and toughness, while providing en.. |
|||
Izod Impact, Notched | 1.40 J/cm @Thickness 4.00 mm, Temperature 23.0 °C |
2.62 ft-lb/in @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Premix Thermoplastics PRE-ELEC® PP 1373 PRE-ELEC PP 1373 is a conductive thermoplastic compound based on polypropylene. Conductivity is achieved by using special conductive carbon black. In addition to a low electrical resistivity PRE-ELE.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | |
Shell Carilon® DB6G6A10 Polyketone, 30% Glass-Reinforced General-Purpose Injection Molding Grade
(discontinue Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer DB6G6A10 is a 30 percent short glass-fiber-reinforced, general purpose injection molding grade, wit.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Ineos Nova 8077 High Performance Styrenic Enhanced Polystyrene
(discontinued **) High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature -30.0 °C |
2.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FXD104R PC (Asia Pacific) FXD104R is a Light Diffusion effect, which is part of the VisualFX family. Color Package may affect properties. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) Zytel® 8018HS BKB085 is a 14% glass reinforced, toughened, heat stabilized black polyamide 66 resin.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 0130 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Loxim 330 01HSL Nylon 6 Information provided by Loxim Industries |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
KYDEX® 2200LT Thermoplastic Sheet for Mass Transit Applications Features:Meets flamespread and smoke development requirements listed in 49 CFR 238Excellent formability and fabrication characteristicsAllows for tight tolerance controlsExcellent resistance to graf.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GF 5150 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GM 5250 OC HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | 63.5*12.7*3.2mm, Cut; ASTM D256 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI) Torlon® 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate partic.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP D451 PC (Asia Pacific) LNP* Thermocomp* D451 (or EXTC8141) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good duc.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EXTC8141 PC (Asia Pacific) LNP* Thermocomp* EXTC8141 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | |
Sanyo PELESTAT® NC6321 ABS (12wt%) PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) that give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a va.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D265 |
Solvay TECHNYL® 2412GHF8 PA66, 40% glass fiber, DRY Description: Polyamid 66, reinforced with 40% of glass fiber, heat stabilized for injection moldingAvailable in: Asia PacificProduct Applications: TECHNYL® 2412GHF8 is used in all sectors of indu.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Wellman Wellamid® GF33-66/6 XE-N 33% Glass Fiber Reinforced Nylon 66/6, Lubricated & Heat Stabilized Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Wellman Wellamid® XT1486-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Izod Impact, Notched | 1.40 J/cm @Temperature 23.0 °C |
2.62 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPH307G6 Polypropylene, 30% Glass Fiber 30% glass fiber reinforced, impact modified polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | >= 1.40 J/cm @Thickness 3.17 mm |
>= 2.62 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PP-CP20/2 Impact Copolymer, 20 Melt Flow This product is intended for general purpose injection molding applications including automotive and consumer products, large buckets and pails where toughness and cold temperature impact are requir.. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN SM-1 PTFE Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ISO 180 |
Azoty Tarnow™ TARFLEN ST PTFE Free-Flowing suspension powder for ram extrusion of rods, pipes and other profiles.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Adell BT-17 Nylon 6, 35% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.40 J/cm | 2.62 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Torlon® 4203 Polyamide-imide (PAI)
(discontinued **) Torlon 4203 is an unreinforced, lubricated, pigmented grade of polyamide-imide (PAI) resin for extrusion. It has the best impact resistance and greatest elongation of all the Torlon grades. Torlon P.. |