Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Asia Pacific) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
Izod Impact, Notched | 6.87 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP1HF PC Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Izod Impact, Notched | 6.87 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Izod Impact, Notched | 6.87 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
12.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® TE5000G PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Door Garnish, Door Handle)CAS No. 24968-12-5 and 103598-77-2Information provid.. |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
12.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® TE5011M PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional Stability, Good WeatherabilityApplication: Automotive (Bumper Back Beam)CAS No. 24968-12-5 and 103598-77-2Information provided by LG .. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature 23.0 °C |
12.9 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-20UVR30 Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household ap.. |
|||
Izod Impact, Notched | >= 6.86 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 12.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN1002FC PC, Halogen Free, Flame Retardant, High Impact Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2, 25232-40-0 and 139189-30-3Information .. |
|||
Izod Impact, Notched | >= 6.86 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 12.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GN1006FL PC, Halogen Free, Flame Retardant, Transparency Description: Injection Molding, PC, Halogen Free Flame Retardant, TransparencyApplication: IT/OA, Electric & Electronic Housing and ComponentsCAS: 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 6.86 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 12.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP1000L PC, Transparent Description: Injection Molding, PC, General Purpose, Transparency, High FlowApplication: IT/OA, E&E Housing and Components Automotive InteriorCAS: 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 6.86 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 12.9 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY SC5004T PC/Polyester, Transparency Description: Injection Molding, PC/Polyester, General Purpose, Transparency, High FlowApplication: Keypad for Mobile PhoneCAS: 103598-77-2Information provided by LG Chemical |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU) Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins... |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU) Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha.. |
|||
Izod Impact, Notched | 6.87 J/cm @Temperature -20.0 °C |
12.9 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 1105 PBT+PC (Asia Pacific) PBT/PC blend, injection molding grade, non-reinforced, impact modified, excellent toughness at low temperatures, very good paintability |
|||
Izod Impact, Notched | 6.91 J/cm @Temperature 0.000 °C |
12.9 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 67001XXH PBT+PC LNP* THERMOCOMP* 67001XXH is a compound based on PC + PBT resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added featu.. |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GW-1041 PC/ABS, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GW-1041 PC/ABS, Unreinforced Recycled Eco-friendly Post-Consumer recycled content.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 6.86 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samyang Trirex® 3017IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017IR is a super high flow grade with added heat stabilizers, separating materials and.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.20 mm |
12.9 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Bayblend® T 85 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
Izod Impact, Notched | 6.86 J/cm | 12.9 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® H24WC High Toughness Heat Strength PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Izod Impact, Notched | 6.86 J/cm | 12.9 ft-lb/in | ASTM D256 |
Asia Technology Pioneers CAP 502 PP Nanocomposite Description: CAP502 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Izod Impact, Notched | 6.86 J/cm | 12.9 ft-lb/in | ASTM D256 |
E-Polymers TEKALOY® G75NHT Brominated Flame Retardant High Impact PC/ABS Alloy PC/ABS, PC/PBT, PC/PET: TEKALOY is high performance polymer alloy resins (PC/ABS, PC/PBT, and PC/PET, etc) manufactured by E-Polymers. PC/ABS has excellent mechanical properties, high heat resistan.. |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® S630X , High Impact, Weather Resistance, Chemical Resistance PC/PBT Alloy High impact, weather resistance, chemical resistanceInformation provided by E-Polymers Co. Ltd. |