Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Mytex Polymers AS33L-07V Polypropylene, Rubber modified, Compounded Description: AS33L-07 is a compounded, rubber modified polypropylene with good impact and excellent material flow properties. This product is designed for painted and mold-in-color applications.Key.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Asia Pacific) LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Europe-Africa-Middle East) LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2000 PC Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BPL1000 PC Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® BFL2000 PC (Europe-Africa-Middle East) Non-Brominated, non-chlorinated flame retardant PC. Available in opaque white colors. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
LATI LASTANE 50 G/40 40% Glass Fiber Reinforced Polyurethane (PUR)
(discontinued **) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Izod Impact, Notched | 6.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.2 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH830 Flame Retardant PC Features:UL V-0 @ 1.6mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surfaceApplications:Controller switchLamp-chimneyTelecommunicationHousehold appliance cabinetInformation Prov.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 23.0 °C |
11.2 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX IN-5001 High Impact PBT LUMAX resins are a family of thermoplastic blends of polybutyleneterephthalate(PBT) and styrenic resins that combine the most desirable properties of both resins and fillers. They offer high heat r.. |
|||
Izod Impact, Notched | 5.98 J/cm @Temperature -40.0 °C |
11.2 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® 5720U PBT+PC (Europe-Africa-Middle East) Unfilled PBT+PC alloy. Outstanding low temperature impact/chemical resistance. UV stabilized version of XENOY |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 0.000 °C |
11.2 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 0.000 °C |
11.2 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Asia Pacific) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 0.000 °C |
11.2 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East) Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature 0.000 °C |
11.2 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC (Asia Pacific) Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature -30.0 °C |
11.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific) Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing.. |
|||
Izod Impact, Notched | 6.00 J/cm @Temperature -30.0 °C |
11.2 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC (Europe-Africa-Middle East) Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SPS Guang Zhou POLOYâ„¢ 2002(+) Flame-retarded PC/ABS Characteristic: Good flame retardance, good mechanical properties and good machining propertiesApplications: Communication products, audio and video productsInformation Provided by SPS (Guang Zhou) .. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP NX10302 PC+ABS (Asia Pacific) This is a PC/ABS compound with improved plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ISO 180/4A |
Styron CALIBREâ„¢ 280-15 Polycarbonate CALIBREâ„¢ PC Utility Grade 280-15 is a high flow opaque polycarbonate with an internal mold release system. Applications: Internal parts Electrical Electronics Lightning Information provided b.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2173HU Toyota High Impact Copolymer Polypropylene DescriptionPolyfort® PP 2173HU Toyota is a high flow, UV stabilized, high impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.98 J/cm | 11.2 ft-lb/in | ASTM D256 |
Aclo Accuguard Polypropylene CP0467V2CSL Copolymer Flame Retardant Copper Stabilized |
|||
Izod Impact, Notched | 6.00 - 9.00 J/cm @Temperature 23.0 °C |
11.2 - 16.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Kleerdex Kydex® 1900 Acrylic/PVC Thermoplastic Sheet
(discontinued **) Mid-temperature aircraft gradeApplications: This sheet product is designed for use in small aircraft interiors but also is appropriate for other applications where higher in-service temperatures may.. |
|||
Izod Impact, Notched | 6.00 J/cm | 11.2 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Asia Pacific) Cycoloy Medium Heat Plating Grade for Automotive |