| Category | Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant |
| Manufacturer | Aclo Compounders |
| Trade Name | Accuguard |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Aclo Accuguard Polypropylene CP0467V2CSL Copolymer Flame Retardant Copper Stabilized.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 0.960 g/cc | 0.0347 lb/in³ | ASTM D792 |
| Linear Mold Shrinkage | 0.013 cm/cm | 0.013 in/in | MD; ASTM D955 |
| Melt Flow | 6.0 g/10 min | 6.0 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 69 | 69 | ASTM D785 |
| Tensile Strength at Break | 18.0 MPa | 2610 psi | ASTM D638 |
| Tensile Strength, Yield | 24.0 MPa | 3480 psi | ASTM D638 |
| Elongation at Break | 75 % | 75 % | ASTM D638 |
| Elongation at Yield | 6.0 % | 6.0 % | ASTM D638 |
| Tensile Modulus | 1.150 GPa | 166.8 ksi | ASTM D638 |
| Flexural Strength | 28.0 MPa | 4060 psi | ASTM D790 |
| Flexural Modulus | 1.150 GPa | 166.8 ksi | ASTM D790 |
| Izod Impact, Notched | 5.98 J/cm | 11.2 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 77.2 °C | 171 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 50.0 °C | 122 °F | |
| Flammability, UL94 | V-2 @Thickness 1.59 mm |
V-2 @Thickness 0.0625 in |
UL File #E99379(N) |