Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR33 Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |
|||
Izod Impact, Notched | 1.03 J/cm @Temperature -30.0 °C |
1.93 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Izod Impact, Notched | 1.03 J/cm @Temperature -30.0 °C |
1.93 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Asia Pacific) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Izod Impact, Notched | 1.03 J/cm @Temperature -30.0 °C |
1.93 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® CFR9111 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9111 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.5 mm and good flow capability. .. |
|||
Izod Impact, Notched | 1.03 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.93 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 1.03 J/cm @Thickness 3.20 mm |
1.93 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
LG Chemical LUMILOY GP2200 Injection Molding Grade, General Purpose 20% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Flow, High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts wi.. |
|||
Izod Impact, Notched | 1.03 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.93 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa FRHIPSV-0 Flame Retardant Polystyrene Features:UL 94 V-0 @ 1.6mm, V-0 @ 3.2mmExcellent balance propertiesHigh mechanical strengthGood heat stabilityColor tailor-made for clientApplications:Injection moldingGas assistant moldingTV or aud.. |
|||
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP IFL36L PA6.12 LNP* LUBRICOMP* IFL36L is a compound based on Nylon 6/12 containing 30% Glass Fiber, 15% PTFE. Added features of this grade include: Low Extractable, Wear Resistant. |
|||
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP LFL36E PEEK LNP* LUBRICOMP* LFL36E is a compound based on Polyetheretherketone containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Wear Resistant, Easy Molding. |
|||
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP QFN16 PA 6/10 LNP* LUBRICOMP* QFN16 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber, 5% MOS2. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON RE007 PA 66 LNP* STAT-KON* RE007 is a compound based on PA66 resin containing 35% Carbon Fiber. Added features include: Electrically Conductive. |
|||
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MX00709 PP LNP* THERMOCOMP* MX00709 is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this grade are: Heat Stabilized, UV Stabilized. |
|||
Izod Impact, Notched | 1.03 J/cm @Temperature -30.0 °C |
1.93 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GFN1 PPE+PS PPE+PS blend. 10% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Izod Impact, Notched | 1.03 J/cm @Thickness 3.17 mm |
1.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika AXG-1500-300 Conditioned Characteristics: Glass-reinforced grades of the AX1500 resin, excellent in heat and chemical resistancesFavorable rigidity and dimensional accuracyInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N6G45 Nylon 6, 45% Glass Filled |
|||
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® HG20L 20% Glass Fiber Reinforced High Impact PA/ABS Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.H-series: PA6/ABS, PA66/AB.. |
|||
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256 |
Cheng Yu Plastic ML3415 PC, 15% Glass Fiber |
|||
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL GTX CRN730V PPE+PA6 (Asia Pacific) PPE+PA+GF, FR |
|||
Izod Impact, Notched | 1.03 J/cm | 1.93 ft-lb/in | ASTM D256A |
Sumitomo Bakelite North America FM 7700P Fiberglass and Mineral Reinforced Phenolic Novolac FM 7700P is a two-stage phenolic molding compound reinforced with cotton fabric in pellet form. FM-7700P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-20. (Replaces Mil.. |