Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.747 J/cm @Temperature 23.0 °C |
1.40 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products GC30P100-01UV 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV Stabilized, Black Applications: Exterior automotive componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.747 J/cm @Temperature 22.8 °C |
1.40 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources TP-G20 Polybutylene Terephthalate, 20% Glass Reinforced Polybutylene Terephthalate, 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information prov.. |
|||
Izod Impact, Notched | 0.747 J/cm | 1.40 ft-lb/in | ASTM D256 |
Ravago Manufacturing Americas Hylon® N1025HLFRA Nylon 66, 25% Glass Filled Nylon 66, 25% Glass Filled, Heat Stabilized, Lubricated, RoHS Compliant, Flame RetardantInformation provided by Ravago. |
|||
Izod Impact, Notched | 0.747 J/cm | 1.40 ft-lb/in | 73°F; ASTM D256 |
Ravago Manufacturing Americas Hylon® N2040MGHL Nylon 6 (DAM) Information provided by Ravago. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.40 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Stat-Tech™ PK-30NCF/10T PEEK - 30% Nickel Coated Carbon Fiber - 10% PTFE
(discontinued **) Data provided by PolyOne. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 3.18 mm |
1.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® UC-1006 Polyphthalamide, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 3.17 mm |
1.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PES GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 3.17 mm |
1.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® TPX-PA6/6-95001 Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.747 J/cm @Thickness 3.17 mm |
1.40 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PBT/ABS GF/M40 FR 40/40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral Fiber Reinforcement, 40/40% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.747 J/cm @Temperature 22.8 °C |
1.40 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Teknor Apex Sinpolene GPP1620 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 20% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Izod Impact, Notched | 0.747 J/cm | 1.40 ft-lb/in | 0.125 in; ASTM D256 |
Chase Plastics CP Pryme® A120 ABS, 20% Glass Fiber Reinforced Features: Glass fiber reinforcementInjection moldingForm: PelletsInformation provided by Chase Plastics. |
|||
Izod Impact, Notched | 0.747 J/cm @Temperature 0.000 °C |
1.40 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Formosa Plastics Formolene® 2510W Medium Impact Copolymer Polypropylene Impact CopolymerApplications: Trans-white battery casesFormolene 2510W is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dime.. |
|||
Izod Impact, Notched | 0.747 J/cm @Temperature 22.8 °C |
1.40 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Clariant Renol ABNN732017 Nylon 6 with anchored silicone Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 0.747 J/cm | 1.40 ft-lb/in | ASTM D256 |
Aclo Accutech Polypropylene Copolymer CP0436M30L Mica Reinforced |
|||
Izod Impact, Notched | 0.747 J/cm | 1.40 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F; ASTM D648 |
PolyOne Edgetek® ES-10GF/000 PES (Polyethersulfone), 10% Glass Reinforced, Hi-Temp
(discontinued **) Information provided by PolyOne™ Corporation |
|||
Izod Impact, Notched | 0.747 J/cm | 1.40 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer
(discontinued **) XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder tempe.. |
|||
Izod Impact, Notched | 0.747 J/cm | 1.40 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® LH5204 Injection Molding HDPE
(discontinued **) CopolymerApplications: Pails, lids and over-capsFormolene LH5204 is a high density polyethylene for injection molding applications.Meets all requirements of the U.S. Food and Drug Administration as .. |