Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
PolyMirae Moplen 341R Injection Molding Grade Polypropylene Moplen RP341R is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP341R is a random copolymer particularly suitable for injecti.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
PolyMirae Moplen HF550K Stretch/Yarn, Monofilament Grade Polypropylene Moplen HF550K is the ADDIFORM polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Its appearance is spherical, white particle with diameter of 1mm .. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
PolyMirae Moplen RP340R Injection Molding Grade Polypropylene Moplen RP340R is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340R is a random copolymer particularly suitable for injecti.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Kolon KOCETAL® K300LO Low Odor Acetal Resin Low odor of formaldehyde gas. Applications: Products for low odor. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GN1001AF PA6, Halogen Free Flame Retardant Feature: Injection Molding, PA6, Halogen Free Flame RetardantApplication: Electrical & Electronic (Switch)CAS No. 25038-54-4 and 37640-57-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP3200A(W) PA6+MF20%, General Purpose Feature: Injection Molding, PA6+MF23%, High ImpactPA6+MF15%, General PurposeApplication: E&E (Rice Cooer Housing)CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP1000FC Flame Retardant PP Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Kolon SPESIN® KP270 General Purpose PBT Base Resin Excellent extrudabilityApplications: CablesInformation provided by API-Kolon. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOS GP-2201F General Purpose ABS, 20% Glass Fiber Reinforced, Flame Retardant LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have .. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY SG5009F PC/ABS Description: Injection Molding, PC/ABS, High Gloss, Scratch Resistance, Halogen Free Flame RetardantApplication: IT&OA (Notebook PC & Monitor housing)CAS: 103598-77-2 and 181028-79-5Information prov.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC M1700 Polypropylene Impact Copolymer Features: SEETEC M1700 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1700 exhibits a very high flowability and a good balance of stiffness and impact strength.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene 2511PCX TA6 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 30% TALCUM REINFORCED HIGH IMPACT STRENGTHAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
|
Kuraray SEPTON® CM1 Compatibilizer Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL TPN9221 PPE+PS (Asia Pacific) Transparent Noryl grade with 90dc and V-2 FR |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -30.0 °C |
0.918 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® AB9515 ABS+PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQNH4550 PBT (Asia Pacific) Valox* iQNH4550 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% based on EPEAT.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | |
Shinil Chemical SHINCON PA66 Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | |
Shinil Chemical SHINCON PPS-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | |
Shinil Chemical SHINSTAT PE Electrostatic Control Polymer Sheet Grade SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for .. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NF-3017 PC/ABS, Unreinforced FR Flame-retardant scratch resistant material that can be used in notebook B partInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NF-3017 PC/ABS, Unreinforced FR Flame-retardant scratch resistant material that can be used in notebook B partInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL NC220 PPE+HIPS (Asia Pacific) |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX2949 PPE+PS (Asia Pacific) PPE+PS GF+Mineral Filler total 40% |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
UBE UBESTA® 3014U Rigid Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | ASTM D256 |
Daelim H&L Plavis-G15 ISO 15% Graphite Filled Aromatic Polyimide Bearing Isostatically Molded. Plavis-G-15: Graphite 15 wt% filled, Self lubricating grade for wear and friction applications.General Plavis information for all grades:PLAVIS polyimide has nitrogen bonded .. |
|||
Izod Impact, Notched | 0.490 J/cm | 0.918 ft-lb/in | Dry; ASTM D256 |
Asahi Kasei Leona® 1700S Nylon 66 Similar to 1500 but with even higher molecular weight. Suitable for extrusion of thick-wall parts.Applications:Rods, films Information provided by Asahi Kasei |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
0.918 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 6010FEN Nylon 66 Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene 2563PCX TA6 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 30% TALCUM REINFORCED HIGH IMPACT STRENGTH, CONTAIN UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |