Material Notes:
LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since both materials cost high, there is a need to design the material with cost effectiveness. Also, the current LCD Rack has a concern of sloughing by CF particulates. SHINIL sloves these problems with the CNT composite of polyphenylene sulfide (PPS), polyether sulfone (PES), PEEK, or polyether imide (PEI) by providing the cost effectiveness combined with enhanced mechanical properties. Especially, the wear resistance (coefficient of friction, coefficient of abrasion) of SHINIL CNT composite was much lower than the current PEEK material, which will provide the material for clean/dust free LCD operation environments.Features and BenefitsPermanent electro conductivityImproved mechanical propertiesNo particulates and no sloughingLighter weightRecyclabilityLow abrasion and frictionImproved surfaceCost effectiveInformation Provided by Shinil Chemical Industry Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 98.1 MPa
14200 psi
Flexural Strength 225.63 MPa
32725 psi
Flexural Modulus 20.6 GPa
2990 ksi
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
Coefficient of Friction, Dynamic 0.3081

@Time 3600 sec,
Pressure 1.96 MPa
0.3081

@Time 1.00 hour,
Pressure 284 psi
0.2 m/s
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 275 °C
527 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+7 ohm-cm
2.00e+7 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 290 °C
554 °F
Descriptive Properties Value Comments
Abrasion Weight (g) 0.0004
Wear Tester 0.2m/s; 20kgf/cm<sup>2</sup>; 1hr
Coefficient of Abrasion (10-3 cm2-sec/kgf-m-hr) 0.0279
Wear Tester 0.2m/s; 20kgf/cm<sup>2</sup>; 1hr