Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.190 J/cm | 0.356 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycolac® INP630 ABS+SAN INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi.. |
|||
Izod Impact, Notched | 0.190 - 0.240 J/cm | 0.356 - 0.450 ft-lb/in | ASTM D256 |
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu.. |
|||
Izod Impact, Notched | 0.190 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.356 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips EA3350 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical containersBlends with clear SB-copolymersClam-shell containersBi-axially oriented sheetFeatures:High molecular weight homopolymerHigh Vicat softeni.. |
|||
Izod Impact, Notched | 0.190 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.356 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips MC3200 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Medical partsConsumer containers, vials, jars, etc.Clock lensesAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat softening tempera.. |
|||
Izod Impact, Notched | 0.190 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.356 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips MC3600 Crystal Polystyrene
(discontinued **) General purpose crystal polystyrene.Applications:HousewaresConsumer containers, vials, jars, etc.Disposable cutleryInjection molded drink cupsFeatures:Easy filling of thin-walled partsExceptional mo.. |
|||
Izod Impact, Notched | 0.190 - 2.10 J/cm @Temperature -40.0 - -40.0 °C |
0.356 - 3.93 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 1.86 J/cm Grade Count:12 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Izod Impact, Notched | 0.190 - 2.10 J/cm @Thickness 3.20 - 3.20 mm |
0.356 - 3.93 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 1.86 J/cm Grade Count:12 |
Overview of materials for ECTFE Fluoropolymer This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Izod Impact, Notched | 0.190 - 0.271 J/cm | 0.356 - 0.508 ft-lb/in | Average value: 0.224 J/cm Grade Count:3 |
Overview of materials for Phenolic, Resole, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v.. |
|||
Izod Impact, Notched | >= 0.190 J/cm | >= 0.356 ft-lb/in | Method A; ASTM D 256 |
Karina 805-18/105-IS-SD Gray PVC Compound Packaging Grade PVCInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.190 J/cm | 0.356 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON EX02598C PEI LNP* STAT-KON* EX02598C is a compound based on Polyetherimide containing Proprietary Filler(s). Added features of this material include: Clean Compound System, Electrically Conductive. |
|||
Izod Impact, Notched | 0.190 J/cm | 0.356 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON FD000 PE LNP* STAT-KON* FD000 is an unfilled Polyethylene. Added feature of this grade is: Electrically Conductive. |
|||
Izod Impact, Notched | 0.190 J/cm | 0.356 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WH0270F PBT LNP* Thermocomp* WH0270F is a dense compound based on PBT. |
|||
Izod Impact, Notched | 0.190 J/cm | 0.356 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 8398 Hardware Grade Epoxy Fiberglass and mineral reinforced epoxy molding compound with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Vyncolit, a Sumitomo B.. |
|||
Izod Impact, Notched | 0.190 J/cm | 0.356 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 8940SG Electrical Encapsulation Grade Epoxy Mineral reinforced epoxy molding compound formulated for the encapsulation of electronic devices requiring high quality, exceptional reliability, and outstanding moldability. USES: Passive electron.. |
|||
Izod Impact, Notched | 0.190 J/cm | 0.356 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America E 16521A Electrical Encapsulation Grade Epoxy E-16521A is an encapsulation grade epoxy molding compound suitable for electrical applications such as coils.Information provided by Sumitomo Bak North America, Inc. |
|||
Izod Impact, Notched | 0.190 J/cm @Temperature 23.0 °C |
0.356 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WH0270FX_WH5A289 PBT 2.7 specific gravity PBTThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.190 J/cm @Thickness 3.20 mm |
0.356 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SC 202EL General Purpose Polystyrene CharacteristicsHigh strength grade Excellent process ability Reduces processing cycle timeProcessing MoldingApplicationsAudio cassettes housing and covers, CD jewel boxes Medical products like disp.. |
|||
Izod Impact, Notched | 0.190 J/cm | 0.356 ft-lb/in | ASTM D256 |
Plenco 4527 Phenolic, Granular, Injection Molded PLENCO 04527 is a heat resistant, mineral and flock filled phenolic molding compound, offering excellent mechanical strength, and resistance to cracking in a wet-dry environment. UL recognized under.. |
|||
Izod Impact, Notched | 0.190 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.356 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips MB3150 Crystal Polystyrene High heat crystal polystyrene.Applications:Compact disc jewel boxesConsumer containers, vials, jars, etc.Desk organizersAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat sof.. |
|||
Izod Impact, Notched | 0.190 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.356 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips MC3650 Crystal Polystyrene General purpose crystal polystyrene.Applications:HousewaresConsumer containers, vials, jars, etc.Disposable cutleryInjection molded drink cupsFeatures:Easy filling of thin-walled partsExceptional mo.. |
|||
Izod Impact, Notched | 0.190 J/cm @Temperature 23.0 °C |
0.356 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 107 Injection Molding Polypropylene Applications: Thin-walled parts and easy mould filling. Information provided by Braskem |
|||
Izod Impact, Notched | 0.190 - 0.240 J/cm | 0.356 - 0.450 ft-lb/in | ASTM D256 |
3D Systems Accura® 25 Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el.. |
|||
Izod Impact, Notched | 0.190 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
0.356 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips EA3025 Crystal Polystyrene
(discontinued **) High heat crystal polystyrene.Applications:Foam egg cartonsFoam meat traysInsulation boardBi-axially oriented sheetFeatures:Ultra-high molecular weight homopolymerHigh Vicat softening temperatureNar.. |