Mechanical Properties Metric English Comments
Izod Impact, Notched 0.534 - 1.07 J/cm
1.00 - 2.00 ft-lb/in
PolyChem Alloy PolyOxyter 2501
PolyOxyter, an additive masterbatch product, has been specially formulated with reactive compounds to provide performance enhancement and processing improvement for Polyesters, Nylons, and Polycarbo..
Izod Impact, Notched 0.534 - 1.07 J/cm
1.00 - 2.00 ft-lb/in
PolyChem Alloy PolyOxyter 5001
PolyOxyter, an additive masterbatch product, has been specially formulated with reactive compounds to provide performance enhancement and processing improvement for Polyesters, Nylons, and Polycarbo..
Izod Impact, Notched 0.214 - 1.07 J/cm
0.400 - 2.00 ft-lb/in
Average value: 0.492 J/cm Grade Count:21
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Izod Impact, Notched 0.235 - 1.07 J/cm
0.440 - 2.00 ft-lb/in
Average value: 0.689 J/cm Grade Count:78
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Izod Impact, Notched 0.235 - 1.07 J/cm
0.440 - 2.00 ft-lb/in
Average value: 0.641 J/cm Grade Count:22
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..
Izod Impact, Notched 0.534 - 1.07 J/cm
1.00 - 2.00 ft-lb/in
Average value: 0.749 J/cm Grade Count:9
Overview of materials for PEKK, Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Notched 0.800 - 1.07 J/cm

@Thickness 6.35 mm
1.50 - 2.00 ft-lb/in

@Thickness 0.250 in
ASTM D256
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE  (discontinued **)
Data provided by PolyOne.
Izod Impact, Notched 1.01 - 1.07 J/cm

@Temperature -20.0 - -20.0 °C
1.89 - 2.00 ft-lb/in

@Temperature -4.00 - -4.00 °F
Average value: 0.864 J/cm Grade Count:2
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Izod Impact, Notched 1.01 - 1.07 J/cm

@Thickness 3.18 - 3.18 mm
1.89 - 2.00 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.864 J/cm Grade Count:2
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..
Izod Impact, Notched 0.534 - 1.07 J/cm
1.00 - 2.00 ft-lb/in
Average value: 0.839 J/cm Grade Count:7
Overview of materials for Polycarbonate/Polysulfone Alloy
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polysulfone Alloy". Each property range of values reported is minimum and maximum values o..
Izod Impact, Notched 0.534 - 1.07 J/cm

@Temperature 0.000 - 0.000 °C
1.00 - 2.00 ft-lb/in

@Temperature 32.0 - 32.0 °F
Average value: 0.668 J/cm Grade Count:4
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Notched 0.534 - 1.07 J/cm

@Thickness 3.18 - 3.18 mm
1.00 - 2.00 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.668 J/cm Grade Count:4
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
Izod Impact, Notched 0.534 - 1.07 J/cm
1.00 - 2.00 ft-lb/in
Average value: 0.835 J/cm Grade Count:19
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E..
Izod Impact, Notched 0.961 - 1.07 J/cm
1.80 - 2.00 ft-lb/in
Average value: 1.00 J/cm Grade Count:5
Overview of materials for Polyetherimide (PEI), 40% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 40% Glass Fiber". Specific grades with glass content between 35% and 44% are included. E..
Izod Impact, Notched 0.801 - 1.07 J/cm
1.50 - 2.00 ft-lb/in
Average value: 0.921 J/cm Grade Count:4
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 0.196133 - 1.07 J/cm

@Temperature -30.0 - -30.0 °C
0.367438 - 2.00 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.377 J/cm Grade Count:11
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Izod Impact, Notched 0.196133 - 1.07 J/cm

@Thickness 3.17 - 6.40 mm
0.367438 - 2.00 ft-lb/in

@Thickness 0.125 - 0.252 in
Average value: 0.377 J/cm Grade Count:11
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
Izod Impact, Notched 0.374 - 1.07 J/cm
0.700 - 2.00 ft-lb/in
Average value: 0.807 J/cm Grade Count:10
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
Izod Impact, Notched 0.320 - 1.07 J/cm
0.599 - 2.00 ft-lb/in
Average value: 0.505 J/cm Grade Count:13
Overview of materials for Nylon 612, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp..
Izod Impact, Notched 0.427 - 1.07 J/cm
0.800 - 2.00 ft-lb/in
Average value: 0.532 J/cm Grade Count:15
Overview of materials for Nylon 612 with PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612 with PTFE Filler". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Notched 0.534 - 1.07 J/cm
1.00 - 2.00 ft-lb/in
Average value: 0.849 J/cm Grade Count:10
Overview of materials for Nylon 11 with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are includ..
Izod Impact, Notched 0.667 - 1.07 J/cm
1.25 - 2.00 ft-lb/in
ASTM D256
Buckeye Polymers BP RPPC 1020 TU BLK Polypropylene Copolymer
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis..
Izod Impact, Notched 0.534 - 1.07 J/cm
1.00 - 2.00 ft-lb/in
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade
BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co..
Izod Impact, Notched 0.270 - 1.07 J/cm
0.506 - 2.00 ft-lb/in
Average value: 0.534 J/cm Grade Count:27
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Izod Impact, Notched 0.641 - 1.07 J/cm
1.20 - 2.00 ft-lb/in
Average value: 0.822 J/cm Grade Count:18
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% ..
Izod Impact, Notched 0.270 - 1.07 J/cm
0.506 - 2.00 ft-lb/in
Average value: 0.616 J/cm Grade Count:41
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Izod Impact, Notched 0.801 - 1.07 J/cm
1.50 - 2.00 ft-lb/in
ASTM D256
Aaron Industries AAROLENE® ARPS HI 100-3 Polystyrene Compounded Resin
AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified.
Izod Impact, Notched 0.534 - 1.07 J/cm
1.00 - 2.00 ft-lb/in
Average value: 0.714 J/cm Grade Count:11
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..
Izod Impact, Notched 0.534 - 1.07 J/cm
1.00 - 2.00 ft-lb/in
Average value: 0.641 J/cm Grade Count:5
Overview of materials for Polypropylene with Glass Fiber + PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va..
Izod Impact, Notched 0.214 - 1.07 J/cm
0.400 - 2.00 ft-lb/in
Average value: 0.442 J/cm Grade Count:24
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..
Copyright © lookpolymers.com All Rights Reserved