Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.380 - 0.700 J/cm | 0.712 - 1.31 ft-lb/in | Average value: 0.565 J/cm Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass/Mineral Reinforced". Each property range of values rep.. |
|||
Izod Impact, Notched | 0.280 - 0.700 J/cm @Temperature -40.0 - -20.0 °C |
0.525 - 1.31 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.321 J/cm Grade Count:4 |
Overview of materials for Nylon 6, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.500 - 0.700 J/cm | 0.937 - 1.31 ft-lb/in | ASTM D256 |
Loxim 821 02T HB Polypropylene Compound, 20% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.500 - 0.700 J/cm | 0.937 - 1.31 ft-lb/in | ASTM D256 |
Shuman 811 Black Polystyrene Medium Impact Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.500 - 0.700 J/cm | 0.937 - 1.31 ft-lb/in | ASTM D256 |
Shuman 881 Grey Polystyrene Medium Impact Injection molding and extrusion grades, easy processability, good gloss, good surface appearance.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.500 - 0.700 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.937 - 1.31 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM PA 6 GF 30 Polyamide 6, 30% Glass Characteristics: medium viscosity, 30% glass fibre filled |
|||
Izod Impact, Notched | 0.500 - 0.700 J/cm @Thickness 6.35 mm |
0.937 - 1.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT3015 15% Glass Fiber Enforced PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.500 - 0.700 J/cm @Thickness 6.35 mm |
0.937 - 1.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT4815 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.600 - 0.700 J/cm | 1.12 - 1.31 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 155 Phenolic Molding Inorganic and glass fiber Filler, Compression Molded Characteristics:Shock resistantElectrical low lossHigh mechanical strengthHeat stableHigh electrical insulationDimensional stabilityGood mechanical tension bearing strengthGood copper adhesion Color.. |
|||
Izod Impact, Notched | 0.500 - 0.700 J/cm @Thickness 6.35 mm |
0.937 - 1.31 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Chang Chun Plastic PBT4115 Fire Retardant & 15% Glass Fiber Enforced Grade PBT Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.600 - 0.700 J/cm @Temperature -30.0 - 0.000 °C |
1.12 - 1.31 ft-lb/in @Temperature -22.0 - 32.0 °F |
Average value: 0.692 J/cm Grade Count:1 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Izod Impact, Notched | 0.600 - 0.700 J/cm @Thickness 3.20 - 3.20 mm |
1.12 - 1.31 ft-lb/in @Thickness 0.126 - 0.126 in |
Average value: 0.692 J/cm Grade Count:1 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |