Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 8.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 01FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 8.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 13FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 8.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Trilliant™ HC X THC 1101 Natural Copolyester Trilliant™ HC high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Tri.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2200-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2203-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2204-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2205-30 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-30 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2207-22 CR-SX Fiberglass Reinforced Thermoset SMC Premi-Glas® 2207-22 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 3200-30 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-30 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® IFX3420Z PC (Asia Pacific) Lexan* IFX3420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm.. |
|||
Izod Impact, Notched | 8.50 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
15.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Edgetek® XT X XT 1001 Natural Copolyester Edgetek™ XT high performance blends offer outstanding strength, durability and chemical resistance through the combination of Eastman Tritan™ copolyester with other various polymeric resins. Edget.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Asia Pacific) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® ML7689 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7689 polycarbonate (PC) siloxane copolymer resin IS a high viscosity injection molding (IM) grade WITH good processability, offering opportunities FOR shorter IM CYCLE times compared TO sta.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D4812 |
Solvay Specialty Polymers KetaSpire® KT-880 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-880 GF30 is the high-flow, 30% glass-fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
Rostone Rosite® C200BS ESD SMC, Conductive Thermoset Polyester, 10% Glass Reinforced
(discontinued **) Key Features: Electrostatic DissipativeRosite Conductive C used in applications such as molded paper guides in printers and plotters. Conductive C is the UL recognition.Information provided by Onei.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
Ineos K54-05 HDPE K54-05 is a high molecular weight, high density polyethylene copolymer developed for large-part blow molding (drum market) where the finished product demands outstanding physical performance. This m.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256A |
LyondellBasell Hifaxâ„¢ ETA-3131E Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good practical impact, good processabilityApplications: molded.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256A |
LyondellBasell Hifaxâ„¢ ETA-3131EUV Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, UV-stabilized, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good practical impact, good processability, exc.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics XYLEX X7509HP PC+POLYESTER (Europe-Africa-Middle East) PC+Polyester alloy. Houseware applications. USA/Europe Food contact. this grade will no longer be supported with biocompatibility information and should not be used for medical applications which r.. |
|||
Izod Impact, Notched | 8.50 J/cm @Temperature 23.0 °C |
15.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 200-14 Polycarbonate Resin Overview: CALIBREâ„¢ 200-14 polycarbonate resin is a natural, FDA compliant, 14 melt flow rate general purpose polycarbonate resin with no mold release or UV stabilizer.Govt. and Industry Standar.. |
|||
Izod Impact, Notched | 8.50 J/cm @Temperature 23.0 °C |
15.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 2061-6 Polycarbonate Resin Overview: CALIBREâ„¢ 2061-6 resin is suitable for steam and ethylene oxide sterilization required by the health care industry. CALIBRE 2061-6 provides excellent heat resistance, impact strength, .. |
|||
Izod Impact, Notched | 8.50 J/cm @Temperature 23.0 °C |
15.9 ft-lb/in @Temperature 73.4 °F |
ISO 180/4A |
Styron CALIBREâ„¢ 303V-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-15 Series Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products a.. |
|||
Izod Impact, Notched | 8.50 J/cm @Temperature 23.0 °C |
15.9 ft-lb/in @Temperature 73.4 °F |
ISO 180/4A |
Styron CALIBREâ„¢ 302V-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300V-15 Series Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, optical clarity and meets UL94 V-2 rating. CALIBRE 300V series products a.. |
|||
Izod Impact, Notched | 8.50 J/cm @Temperature 23.0 °C |
15.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip.. |
|||
Izod Impact, Notched | 8.50 J/cm @Thickness 3.20 mm |
15.9 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Makrolon® 6555 Polycarbonate, Injection Grade Medium viscosity, flame retardant injection molding with easy mold release, burning behavior.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG a.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
Adell AD-10 Nylon 66, Ultra High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 8.50 J/cm @Thickness 3.17 mm |
15.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Makrolon® LQ-2847 Polycarbonate, Lens Quality Optical, Mold Release, UV Stabilized
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256-70 |
Budd DSM-949, Diesel Grade SMC, Vinyl Ester, Black
(discontinued **) Used for parts requiring high strength at room temperature, good retention of properties at high temperatures and corrosion resistance, such as diesel engine external body parts.Data provided by the.. |
|||
Izod Impact, Notched | 8.50 J/cm | 15.9 ft-lb/in | ASTM D256 |
Rostone Rosite® 4030FS SMC Thermoset Polyester, 30% Glass Reinforced
(discontinued **) Key Features: "Zero Shrink" Grade±1/4 mil shrinkage. Provides surface smoothness for uses such as auto headlamp retainers. High impact and flexural strength combined with dimensional accuracy.Inf.. |