Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® EXCY0025 PC+ABS Recyle Material with PC+ABS+EXL recycle for good low temperature impact performance. |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Asia Pacific) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature -10.0 °C |
12.9 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer (Europe-Africa-Middle East) 19 MFR LEXAN High Flow Ductile Copolymer with 400 nm cut off, available in transparent colors only |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
12.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy) Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert.. |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AFA-6133 V0 Z Polyphthalamide (PPA)
(Unverified Data**) Amodel AFA-6133 V0 Z is a 33% glass-fiber reinforced, flame retardant grade of polyphthalamide (PPA) resin specifically formulated for connector applications requiring compatibility with both infrar.. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature -10.0 °C |
12.9 ft-lb/in @Temperature 14.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® HFD1262 PC Copolymer 19 MFR LEXAN High Flow Ductile Copolymerwith 400 nm cut off, available in transparent colors only |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Bayblend® 2153 Polycarbonate + ABS Blend, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Bayblend® 2753 Polycarbonate + ABS Blend, Automotive
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature 23.0 °C |
12.9 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-20MRA30 Polycarbonate, General Purpose, Mold Release Grade Features: Mold release, Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesIn.. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature 23.0 °C |
12.9 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-20T30 Polycarbonate, General Purpose Features: Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesInformation prov.. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature 23.0 °C |
12.9 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-20UV30 Polycarbonate, General Purpose, UV Stability Grade UV stability, Ultra Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature 23.0 °C |
12.9 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-20UVR30 Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release Super high flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household ap.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
12.9 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
notch |
Kraton® G1650 + PP blend (20/80) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Radel® R-5000 Polyphenylsulfone (PPSU) Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins... |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Radel® R-5100 Polyphenylsulfone (PPSU), Filled Radel® R-5100 is an opaque, general purpose polyphenylsulfone (PPSU) for injection molding, that offers exceptional hydrolytic stability, and toughness superior to other commercially-available, h.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU) Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Radel® R-5600 Polyphenylsulfone (PPSU) Radel® R-5600 is a very high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer excep.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU) Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.18 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Radel® R-5900 Polyphenylsulfone (PPSU) Radel® R-5900 polyphenylsulfone (PPSU) offers medium melt viscosities for long flow lengths and greater injection molding ease. It also provides exceptional hydrolytic stability and toughness tha.. |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 67001XXH PBT+PC LNP* THERMOCOMP* 67001XXH is a compound based on PC + PBT resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added featu.. |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP 67002XXH PBT+PC LNP* THERMOCOMP* 67002XXH is a compound based on PBT+PC containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare applications. Added features inc.. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature 23.0 °C |
12.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 891-10 Polycarbonate Resin Overview: CALIBREâ„¢ 891-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release.. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature 23.0 °C |
12.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256; ISO 180/4A |
Styron CALIBREâ„¢ IM 401-11 Polycarbonate Resin Overview: CALIBREâ„¢ IM 401-11 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy process wi.. |
|||
Izod Impact, Notched | 6.90 J/cm @Temperature 23.0 °C |
12.9 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Styron CALIBREâ„¢ 893-10 Polycarbonate Resin Overview: CALIBREâ„¢ 893-10 Series provides superior ignition resistance in opaque applications. The CALIBRE 891-10 series products are available in 2 additive packages: CALIBRE 891: Mold release.. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.20 mm |
12.9 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Covestro Bayblend® T 85 Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Automotive components, electrical engineering.Information provided by Bayer.As of 1 .. |
|||
Izod Impact, Notched | 6.90 J/cm @Thickness 3.17 mm |
12.9 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Covestro Makrolon® 6255 Polycarbonate, Flame Retardant, High Productivity, Mold Release Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
ABW Polymers PC/PET Alloy Typical property data below. Material may be tailored to meet specific requirements. This data should be used only as a guide and no assurance can be granted by the company that all molded articles.. |
|||
Izod Impact, Notched | 6.90 J/cm | 12.9 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® S630X , High Impact, Weather Resistance, Chemical Resistance PC/PBT Alloy High impact, weather resistance, chemical resistanceInformation provided by E-Polymers Co. Ltd. |