Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 4.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.99 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Compression Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion L7703 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.99 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne OnForce™ LFT UR-60 LGF/000 Natural Polyurethane, Unspecified (PUR, Unspecified) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
Izod Impact, Notched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 3101-22 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-22 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® PPC4701 PPC (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® FXC1200E PC+ABS (Asia Pacific) Visual Fx PC/ABS for strong fluorescent bright colors with good flow, impact and heat resistance characteristics. Consumer electronic and appliance applications uses. |
|||
Izod Impact, Notched | 4.80 J/cm | 8.99 ft-lb/in | Plain Cast Resin; ASTM D256 |
TSE Industries EcoWIND® T211 Filament Winding Polyurethane Resin for Tanks and Pressure Vessels with Thermoplastic Liners TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Izod Impact, Notched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256 |
DuPont™ Surlyn® 8670 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8670 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Izod Impact, Notched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256 |
Glastic Laminates/Shapes UTR Glass-Mat-Reinforced, Mineral Filled Polyester Laminate Data provided by Glastic Corporation.NEMA GPO-3/GPO-3P. Developed for transit industry where smoke generation and toxicity are of primary concern. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
3.2 mm (0.125 in) notch |
Kraton® G1652 + PP blend (20/80) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Izod Impact, Notched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256A |
LyondellBasell Astryn 75A6-2 Polypropylene Copolymer, 20% Calcium Carbonate Key Features: conventional melt flow, medium modulus, mineral-filled polypropylene copolymer, high impact, excellent chemical resistance, excellent aesthetics, high gloss, good colorability, good pr.. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm |
8.99 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2310R PEI 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm |
8.99 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2310R PEI (Asia Pacific) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm |
8.99 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2400 PEI 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm |
8.99 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM 2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm |
8.99 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM AR9100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm |
8.99 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5201 PEI 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm |
8.99 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5201R PEI 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm |
8.99 ft-lb/in @Thickness 0.126 in |
reverse notched; ASTM D 256 |
SABIC Innovative Plastics Ultem CRS5211 PEI 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Th.. |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm |
8.99 ft-lb/in @Thickness 0.126 in |
reverse notched; ASTM D 256 |
SABIC Innovative Plastics Ultem CRS5211 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming, UL94 V0 and 5VA listing.Thi.. |
|||
Izod Impact, Notched | 4.80 J/cm | 8.99 ft-lb/in | ASTM Data |
Styron Magnum™ 9043 ABS, High Gloss Sheet Extrusion Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Izod Impact, Notched | 4.80 J/cm @Temperature -50.0 °C |
8.99 ft-lb/in @Temperature -58.0 °F |
ASTM Data |
Styron Pulse® 1310 ABS + Polycarbonate PULSE® 1310 Engineering resin offers a superior total performance with a balance of heat resistance, practical toughness, high and low temperature impact strength retention and ease of processing.. |
|||
Izod Impact, Notched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON RX04493D PA 66 LNP* VERTON* RX04493D is a compound based on Nylon 66 resin containing proprietary fillers. Added feature of this grade is: Structural. |
|||
Izod Impact, Notched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON RX04493D PA 66 (Asia Pacific) LNP* Verton* RX04493D is a compound based on Nylon 66 resin. |
|||
Izod Impact, Notched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256 |
Covestro Bayflex® 110-50 CM Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and o.. |
|||
Izod Impact, Notched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® PC/ABS Alloy 304 General purpose high gloss with high impact, good low temperature properties and high heat resistance.Data provided by the manufacturer |
|||
Izod Impact, Notched | 4.80 J/cm @Thickness 3.20 mm |
8.99 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
SABIC Innovative Plastics ULTEM AR9100 PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |