Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.00 J/cm @Temperature -30.0 °C |
5.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature -30.0 °C |
5.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Asia Pacific) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature -30.0 °C |
5.62 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® HCX1640 PC+ABS (Europe-Africa-Middle East) CYCOLOY™ HCX1640 a PC+ABS blend specially developed for medical devices and pharmaceutical applications requiring improved mechanical performance . It combines good flow with excellent impact and l.. |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® RCM6134 PC+ABS (Asia Pacific) Cycoloy* RCM6134 resin is an injection moldable filled PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 35% post consumer recycle content with a UL-94 V0 rating @ 1... |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
Radici Heraflex® E 7722 TPC-ET Thermoplastic Elastomer TPC-ET Thermoplastic Elastomer. High Modulus, Nominal Shore D/15s 69. Natural colorProcessing technology: Injection moldingInformation provided by Radici group. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature 23.0 °C |
5.62 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXM4701 PPC LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Americas .. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature 23.0 °C |
5.62 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Asia Pacific) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Asia Paci.. |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
SABIC BM1052 High Density Polyethylene for Blow Molding Product Description: BM1052 grade is a high molecular weight High Density Polyethylene copolymer with broad molecular weight distribution. It has excellent processability and exhibits very high im.. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature 23.0 °C |
5.62 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXM4701 PPC (Europe-Africa-Middle East) LEXAN FMX4701 is a high heat resistant poly(ester)carbonate injection molding resin. This grade is especially designed to visualize color effects.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature 0.000 °C |
5.62 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
Gichem GIBLEND E45400 Polycarbonate / ABS
(discontinued **) Polycarbonate and ABS blend, high fluidity. Medium Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL EC-605B Electrically Conductive POM, 5% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 3.00 - 4.00 J/cm @Temperature 23.0 °C |
5.62 - 7.49 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Loxim 500 00HB Polycarbonate/Acrylonitrile Butadiene Styrene Information provided by Loxim Industries |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS (Asia Pacific) Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS (Asia Pacific) Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL EN7010 PPE+SEBS (Asia Pacific) High heat, Non halogenated flame retardant Noryl product for Film |
|||
Izod Impact, Notched | 3.00 J/cm @Thickness 3.17 mm |
5.62 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Unitika P-3001S Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature 23.0 °C |
5.62 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA830 Nylon 6.6, Impact Modified Impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature 23.0 °C |
5.62 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron P60B04 Homopolymer Polypropylene, Chemically Coupled 60% Long Glass Fiber A CHEMICALLY COUPLED PP 60% LONG GLASS FIBER WITH EXTRA LOAD OF ADDITIVES FOR DILUTION.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM-D256 |
Polyram RamLloy PJ701 ABS/ASA, General Purpose PJ 701 IS A GENERAL PURPOSE INJECTION MOLDING ASA& ABS ALLOY . IT HAS GOOD MECHANICAL PROPERTIES SIMILAR TO ABS AND MUCH BETTER WEATHER RESISTANCE. AN IDEAL ECONOMIC CHOICE.Information provided .. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature 23.0 °C |
5.62 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PV701 ABS, UV Stabilized UV stabilized ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature 23.0 °C |
5.62 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PV801 ABS, Impact Modified Impact modified ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 3.00 J/cm @Temperature 23.0 °C |
5.62 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PV102 ABS, General Purpose General purpose ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | >= 3.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
>= 5.62 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
E-Polymers Tekaloy® G70F2 G70NH, Non-Halogen Flame Retardant, Un-Reinforced PC/ABS Alloy V-2, High FlowInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TA210HI , High Impact Resistance PA66, DAM High impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM-D256 |
Braskem GP5550BK HDPE High Density Extrusion Polyethylene GP5550BK is a high-density polyethylene with high molar mass. It is produced with bimodal technology and shows excellent mechanical properties and high resistance to stress cracking. GP5550BK contai.. |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON UX03320 PPA (Asia Pacific) VERTON* UX03320 is a compound based on Polyphthalamide resin containing Long Glass. |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PX1005X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0/5VA rated. UL746C F1. Excelent dielectric strength. Suitable for E/E market in indoor/outdoor applications. |
|||
Izod Impact, Notched | 3.00 J/cm | 5.62 ft-lb/in | ASTM D256 |
Braskem BU004 Blow Molding High Density Polyethylene Containers for lubricating oils, alcohol, cosmetics and yots; Toys.Information provided by Braskem. |