Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.10 J/cm @Thickness 3.18 mm |
3.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PolyOne Gravi-Tech™ GRV-UR-045-SS-W Black Polyurethane, Unspecified (PUR, Unspecified) Information provided by PolyOne |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ PC-000/05T-2S Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ FR PP FR 8-6 A NATURAL - ROHS Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
3.93 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.17 mm |
3.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Cadon® 127 SMA General Purpose, High Heat
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.93 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JE2-R2 ABS/PBT Alloy Features:Low costExcellent balance propertiesGood processing propertiesGood heat stabilityGood size stabilityGood surfaceApplications:CD-ROM, DVDPrinter, scanner, photocopier cabinetElectric and ele.. |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.17 mm |
3.93 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Lustran® 552 Extrusion, Profile/Substrate Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
Ineos G60-25-144 HDPE Ineos G60-25-144 is a high density polyethylene homopolymer typically used in the production of sheet extrusion and blow molded containers. This material meets the Food and Drug Administration requ.. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | edgewise; ASTM D256 |
Haysite 18600 Polyester BMC, 15% Glass Reinforced The 18600 series bulk molding compound can be compression, transfer, or injection molded. Formulated with a high temperature resin system, this grade exhibits exceptional retention of physical and e.. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | edgewise; ASTM D256 |
Haysite 20000 Polyester BMC, 15% Glass Reinforced The 20000 series bulk molding compound is an electrical grade that can be compression, transfer, or injection molded. Offering good arc/track properties and mechanical strength, this grade is also r.. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256A |
LyondellBasell Higlass SB224-2 Polypropylene Copolymer, 20% Glass Fiber Key Features: conventional melt flow, medium modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high impact strength, moderate rigidity, good processabilityApplications: of.. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
Solvay TECHNYL® eXten D247 F Nylon 66 & 610 Description: Polyamid 66 & 610, impact modified, alkali resistance, mold release, for injection molding. This material is available in natural color and in colors on requestAvailable in: Asia Pacifi.. |
|||
Izod Impact, Notched | 2.10 J/cm @Temperature 23.0 °C |
3.93 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron A30B041 Nylon 66, 30% Long Fiber 30% LONG FIBER GLASS REINFORCED, PTFE LUBRICATED, UV STABILIZED BLACK NYLON 6.6 FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® TB120SG30 Impact Modified, 30% Glass Fiber Reinforced PA6, DAM 30% Glass Fiber reinforced, High impact resistanceInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
Covestro Bayflex® XGT-100 Polyurethane Elastomeric RIM, 15% Milled Glass Filled, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
Buckeye Polymers BP ABS 5425 ABS General PurposeABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of proc.. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
Buckeye Polymers BP ABS 6432 WS ABS ABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing and outs.. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
Adell BJ-37 Nylon 6, 35% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM 3.2mm |
Asahi Kasei Xyron® 450H Modified Polyphenylene Ether Applications: Automotive: Door Handles, Fuse Carriers, Fuse Box Covers, Interior Electrical Outlets, Interior Plugs/Switches, Interior High Precision Parts Electrical and Industrial: Pool and Spa P.. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | |
Buckeye Polymers BP PPC 0412 R Blk Reprocessed Polypropylene, Unfilled BlackThis reprocessed product is successful in applications where cost is a major specification, yet physical characteristics require product performance. Industrial recycled resin compounds are ut.. |
|||
Izod Impact, Notched | 2.10 J/cm @Temperature -40.0 °C |
3.93 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Ashley Polymers Ashlene® 827LD Nylon 6 A very high impact nylon resin for injection molding applications. Outstanding low temperature properties.Data provided by the manufacturer |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | Notched/Unnotched not specified; ASTM D256 |
NOVA Chemicals Novapol® HB-L455-A HDPE Blow Molding Resin
(discontinued **) Molded Plaque Properties. Features: excellent processability on high speed, multiple-head blow molding lines, good balance of physical and molding properties.Applications: chemical bottles, toys.Da.. |
|||
Izod Impact, Notched | 2.10 J/cm @Temperature -40.0 °C |
3.93 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Covestro Bayblend® 2253 Polycarbonate + ABS Blend, Extrusion
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | 2.10 J/cm @Thickness 3.17 mm |
3.93 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8333G HI HS BK-102 33% Glass Filled PA6 (Dry) Ultramid 8333G HI HS BK-102 is a 33% glass reinforced, heat stabilized, impact modified, pigmented black, PA6 injection molding compound developed for applications requiring improved dry as molded t.. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
Adell BJ-17 Nylon 6, 35% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 2.10 J/cm | 3.93 ft-lb/in | ASTM D256 |
Custom Resins Norpex® 2000 PPE (Polyphenylene Ether), 20% Mineral Reinforced