Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP2122G15VO G/F Reinforced & Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMAX HR5157 PBT+ABS+GF15%, Heat Resistance Description: Injection Molding Grade, PBT+ABS+GF15%, Heat ResistanceApplication: E&E (CD ROM Tray)CAS: 9003-56-9, 65997-17-3, 24968-12-5 and 25038-59-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID GP2339B(W) PA66+GF33%, General Purpose Feature: Injection Molding, PA66+GF33%, General PurposeApplication: Automotive (Cylinder Head Cover)CAS No. 32131-17-2 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN177N Nylon Extrusion Resin Excellent transparent & flexible copolyamide, typical applications are fishing nets & fishing linesInformation provided by US distributor, API-Kolon. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP212G30VO G/F Reinforced & Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOS GP2300 ABS+GF30%, General Purpose Feature: Injection Molding, ABS+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-54-7, 9003-56-9 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.785 J/cm @Temperature 23.0 °C |
1.47 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC M1315 Polypropylene Impact Copolymer Features: SEETEC M1315 is a heterophasic polypropylene copolymer for compression molding caps, especially SACMI machines. SEETEC M1315 exhibits an excellent stiffness, a high impact strength, a high.. |
|||
Izod Impact, Notched | 0.785 J/cm @Temperature 23.0 °C |
1.47 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUTENE-H ME6000 HDPE Description: LUTENE-H ME6000 is mainly intended for injection molding of crates. It has excellent mechanical properties and high impact strength.Applications: Transport and stacking crates, bottle c.. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | |
Shinil Chemical SHINCON PEI-CNT LCD Rack LCD Rack is used to transfer or bake LCD frame in the electronic assembly or LCD packaging assembly line. Current LCD Rack is made of poly ether ether ketone (PEEK) with carbon fiber (CF). Since b.. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® T102G30 PET, 30% Glass Filled, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® NH-1101 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4017 ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4020H ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4017 ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4020H ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm |
1.47 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® NH-1904 HIPS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T883GV2 Flame Retardant PBT, 20% Glass Fiber |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
E-Polymers TEKAFIN® PH70G1 HIPP + 10% Glass Fiber Reinforced Scratch Resistance Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
E-Polymers TEKASTER® F10G30 30% Glass Fiber Reinforced PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
E-Polymers TEKAMID® JN930 PPE+PA66 30% Glass Fiber Reinforced PA/PPE Alloy Polyamide (Nylon) Resin. TEKAMID is widely being used in manufacturing of automotive and industrial parts with its outstanding mechanical, thermal and chemical properties.JN-series: PA66/PPE, PA6/P.. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FR200GV25 Flame Retardant Nylon 66, 25% Glass Fiber |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV3010 Polyformaldehyde |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV3015 Polyformaldehyde |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV3020 Polyformaldehyde |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV3025 Polyformaldehyde |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 30G6 Polybutylene terephthalate, 30% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 30G6F Polybutylene terephthalate, 30% Glass Fiber Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 0.785 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.47 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Asia International Enterprise (Hong Kong) 60G4 Nylon 66, 20% Filled Information provided by Asia International Enterprise (Hong Kong) Ltd. |
|||
Izod Impact, Notched | 0.785 J/cm | 1.47 ft-lb/in | ASTM D256 |
E-Polymers SEPAZ® C140GP 40% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |