Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
ASTM D955
Melt Flow 17.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
17.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D785
Tensile Strength, Yield 76.5 MPa
11100 psi
5 mm/min; ASTM D638
Flexural Strength 116 MPa
16800 psi
2.8 mm/min; ASTM D790
Flexural Modulus 5.00 GPa
725 ksi
2.8 mm/min; ASTM D790
Izod Impact, Notched 0.785 J/cm

@Thickness 3.17 mm
1.47 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 100 °C

@Thickness 6.40 mm
212 °F

@Thickness 0.252 in
ASTM D648
Vicat Softening Point 105 °C
221 °F
B/50; ISO R306