Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM UH1006M TPI Blend High heat amorphous TPI Blend, Chemical Resistant |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® X TR2-20TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -30.0 °C |
1.41 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East) XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
SABIC M80064 Series High Density Polyethylene for Injection Molding Product Description: M80064 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Edistir RK Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is suitable for injection moulding. It combines high mechanical strength, heat resistance and good processability.
Designation: Thermopl.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ISO 180/4A |
Polimeri Europa Edistir RKL Polystyrene
(discontinued **) UL94 V-0, flame retarded, high impact polystyrene. This grade is designed for the extrusion of flame retardant sheets, foils and profiles. Designation: Thermoplastics ISO 2897-PS-I,E,093-06-04-18App.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -30.0 °C |
1.41 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JE2-R2G20 Glass Fiber Reinforced ABS/PBT Alloy Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH-R2G10 P60 10% Glass Fiber Reinforced PC/ABS Alloy Features:UL HB @ 1.6-3.2mmExcellent balance propertiesHigh stiffnessGood size stabilityGood surface adhesionExcellent processing properties, large partsApplications:Injection moldingAutomobile instr.. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP-2301F General Purpose PBT, 30% Glass Fiber Reinforced, Flame Retardant LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.17 mm, Temperature -40.0 °C |
1.41 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
ASTM D256 |
Ineos ABS Lustran® 552 Extrusion, Profile/Substrate Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.41 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PBT-RG15 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Izod Impact, Notched | 0.750 J/cm @Thickness 3.18 mm |
1.41 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® BR111 Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® BR111 is a natural-colored glass fiber and mineral filled polyphenylene sulfide compound that provides enhanced mechanical strength with good electrical properties and outstanding chemical.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Veradel® 3430GF Polyethersulfone (PESU), 30% Glass Fiber Veradel® 3430GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 0.000 °C |
1.41 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 865 PBT (Europe-Africa-Middle East) VALOX 865 is a 30% glass fibre reinforced, non blooming flame retardant PBT+PET blend with an excellent surface appearance. Applications: External housings, steam irons, appliance housings and light.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP LC006EXQ PEEK LNP* THERMOCOMP* LC006EXQ is a compound based on Polyetheretherketone containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2175HU Toyota High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU Toyota is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 4529 Mineral Filled Copolymer Polypropylene DescriptionPolyfort® FPP 4528 is a mineral filled copolymer polypropylene for applications requiring good impact and increased stiffness with long term heat stability.Information provided by A. Sch.. |
|||
Izod Impact, Notched | >= 0.750 J/cm @Temperature 23.0 °C |
>= 1.41 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA334G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature 23.0 °C |
1.41 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamShine PW310G13 SAN, 13% Glass Fiber 13% glass fiber reinforced SAN for low warpage and high rigidity injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | >= 0.750 J/cm @Temperature 23.0 °C |
>= 1.41 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA300G6 Nylon 6.6, 30% Glass Fiber 30% glass fiber reinforced polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 2175HU-31 High Flow Copolymer Polypropylene DescriptionPolyfort® PP 2175HU-31 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.750 J/cm @Temperature -40.0 °C |
1.41 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 132 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 653 Nylon 6/6, Carbon Fiber Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.750 J/cm | 1.41 ft-lb/in | ASTM D256 |
Gharda Chemicals Gafone™ B2300 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional properties Transparent Improved Impact Strength and Toughness as compared to PES Excellent Hydorlytic Stability High Stress Cracking Resistance Good Chemical.. |