Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.690 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ X ST6600-0040 ES FR Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.690 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Trilliant™ HC HC5210-0020 RS Natural Polypropylene Homopolymer (PP Homopolymer) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -30.0 °C |
1.29 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY2010 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -30.0 °C |
1.29 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY5000 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering hydrolytic stability and excellent flow for a wide variety of thin wall or large size applicat.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Izod Impact, Notched | 0.690 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PTS Trimid® N6-G15HL 15% GFR Heat Stabilized Nylon 6 with Lube Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature -40.0 °C |
1.29 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Rotuba MS Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
(Unverified Data**) AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C7230P PC+ABS (Asia Pacific) Cycoloy* C7230P resin is a mineral filled, flame retardant PC/ABS. Good stiffness combined with balanced flow and impact performance, makes it a good candidate for various applications. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Udel® P-1720 Polysulfone (PSU)
(discontinued **) Udel P-1720 is a flame-retardant grade of polysulfone (PSU) that has a UL94 rating of V-0 at a thickness of 1 mm (0.039"). In general, polysulfone is a tough, rigid, high-strength thermoplastic that.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Kolon Kopa® KN133HB55 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM AR9100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers KetaSpire® KT-820FP Polyetheretherketone (PEEK) KetaSpire® KT-820FP is the low-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color fine powder form suitable for compression molding. KetaSpire® PEEK is produced.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers PrimoSpire® PR-351 Polyphenylene, Self-Reinforced (SRP) PrimoSpire® PR-351 resin is a higher flow, injection molding grade of PrimoSpire® self-reinforced polyphenylene (SRP). PrimoSpire® SRP resin is an ultra-high performance amorphous, melt-pro.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DEL329XF PC (Asia Pacific) LNP STAT-KON* DEL329XF is a compound based on Polycarbonate resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.690 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp MF006ASJ PP LNP THERMOCOMP* MF006ASJ is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized, Healthcare.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF005SXS PA 66 LNP THERMOCOMP* RF005SXS is a compound based on Nylon 66 resin containing 25% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WF006H PBT LNP* THERMOCOMP* WF006H is a compound based on PBT resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WX88406 Polyester, TP LNP* Thermocomp* WX88406 is a compound based on Polyester, TP resin. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.690 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPC-CC20 Natural Copolymer Polypropylene, 20% Calcium Carbonate Filled Information provided by Entec |
|||
Izod Impact, Notched | 0.690 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled Information provided by Entec |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 435 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 714 PPS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 112 Polypropylene, Glass Reinforced, Chemically Coupled, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.690 J/cm | 1.29 ft-lb/in | Conditioned; ASTM D256 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |