Polymer Property : Izod Impact, Notched = 0.502 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
73°F; ASTM D256
Multibase Multi-Pro® 1508 M Polypropylene
Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Omni Plastics OmniTech™ PA6/6 GR15 MS2 Wear-and-Friction Molybdenum Disulfide filled Nylon
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Solvay Technyl® A218 Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Westlake Plastics Propylux® SD-X7 Polypropylene (static dissipative)
Low carbon black content (1-2%) reduces contamination problems from sloughing - clean room compatible. Also feature low leachable ion levels and low outgassing.Information provided by Westlake Plas..
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accuguard Polypropylene HP0362V0CSL Homopolymer Flame Retardant Copper Stabilized
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334C10L1 Calcium Reinforced
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334C30L Calcium Reinforced
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334C40L Calcium Reinforced
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334G5M25CL Glass/Mineral Reinforced Coupled
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334M10CL Mica Reinforced Coupled
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334M20L Mica Reinforced
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0334M30L Mica Reinforced
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0336C40L1 Calcium Reinforced
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339G20M10CL Glass/Mineral Reinforced Coupled
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Aclo Accutech Polypropylene Homopolymer HP0339G25M5CL Glass/Mineral Reinforced Coupled
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
PlastxWorld Veroplas PA2009L Nylon 6
general purpose, super lubricated injection molding gradeInformation provided by PlastxWorld Inc.
Izod Impact, Notched 0.502 - 8.33 J/cm
0.940 - 15.6 ft-lb/in
Average value: 3.63 J/cm Grade Count:7
Overview of materials for Polypropylene with Carbon Black Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Carbon Black Filler". Each property range of values reported is minimum and maximum v..
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
PlastxWorld Veroplas PA2000 Nylon 6
general purpose, unfilled injection molding gradeInformation provided by PlastxWorld Inc.
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
PlastxWorld Veroplas PA2001F Nylon 6
flame retarded (UL94 VO), unfilled injection molding gradeInformation provided by PlastxWorld Inc.