Aclo Accutech Polypropylene Homopolymer HP0336C40L1 Calcium Reinforced

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Aclo Accutech Polypropylene Homopolymer HP0336C40L1 Calcium Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
MD; ASTM D955
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Ash 39.6 %
39.6 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 84
84
ASTM D785
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D638
Tensile Strength, Yield 26.0 MPa
3770 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Elongation at Yield 4.0 %
4.0 %
ASTM D638
Tensile Modulus 2.099 GPa
304.5 ksi
ASTM D638
Flexural Strength 36.0 MPa
5220 psi
ASTM D790
Flexural Modulus 2.40 GPa
348 ksi
ASTM D790
Izod Impact, Notched 0.502 J/cm
0.940 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 62.2 °C
144 °F