Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.480 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.899 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ AT-000/10T 2S Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.899 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ ATH-XC-361E Acetal (POM) Homopolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Izod Impact, Notched | 0.480 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.899 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ NY-20CF/000 BLACK Polyamide 6 (Nylon 6) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded
&nbs AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)
(Unverified Data**) Udel GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resista.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Kolon KOCETAL® CB301 Conductive Grade Acetal Resin Conductive grade. Applications: Conductive products. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp KP004AXZ Acetal Homopoly LNP* Lubricomp* KP004AXZ is a compound based on Acetal Homopolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP LL003 PEEK LNP* LUBRICOMP* LL003 is a compond based on Polyetheretherketone resin containing 15% PTFE Lubricant. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP OCP34E PPS - Linear (Asia Pacific) LNP LUBRICOMP* OCP34E is a compound based on PPS - Linear resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Easy Molding. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DD000CEX PC (Asia Pacific) LNP* STAT-KON* DD000CEX is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Clean Compounding System. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -30.0 °C |
0.899 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS (Asia Pacific) LNP* Stat-kon* OEL36A is a compound based on Polyphenylene Sulfide resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP EX06430H PEI LNP* THERMOCOMP* EX06430H is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added feature of this grade is: Healthcare. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature 23.0 °C |
0.899 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp IF002 PA 6/12 (Asia Pacific) LNP* Thermocomp* IF002 is a compound based on Nylon 6/12 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1477 Mineral Filled, General-Purpose Polypropylene DescriptionPolyfort® FPP 1477 is a 20% mineral filled, general-purpose polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3711 High Impact Polypropylene DescriptionPolyfort® FPP 3711 is a 26% calcium carbonate filled high impact polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1477 Mineral Filled, General-Purpose Polypropylene DescriptionPolyfort® FPP 1477 is a 20% mineral filled, general-purpose polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm @Temperature -40.0 °C |
0.899 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8202 PA6 (Dry) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 436 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.20% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 197-N2 Acetal A general purpose, very low viscosity, in natural.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 61M Nylon 66, 40% Mineral reinforced A 40% mineral reinforced general purpose Nylon 66 resin with superior stiffness and dimensional stability.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 79MGS Nylon 6, 40% Glass Mineral reinforced A 40% glass mineral reinforced Nylon 6 with good dimensional stability, stiffness, sink and warp resistance. Modified for improved surface appearance.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3454F Talc Filled Copolymer DescriptionPolyfort® FPP 3454F is a 20% talc filled copolymer.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 - 3.52 J/cm | 0.899 - 6.59 ft-lb/in | Average value: 2.02 J/cm Grade Count:22 |
Overview of materials for Cellulose Acetate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate, Molded". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1477 Mineral Filled, General-Purpose Polypropylene DescriptionPolyfort® FPP 1477 is a 20% mineral filled, general-purpose polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DX04490 PC (Asia Pacific) LNP* Stat-kon* DX04490 is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Notched | 0.480 J/cm | 0.899 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2110 PEI 10% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |