Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | >= 9.00 J/cm² | >= 42.8 ft-lb/in² | Partial Break; ISO 179/1eA |
Quadrant EPP Cestilene™ HD 1000 R Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® 1000 ASTL PE-UHMW + specific additives (ISO Data) TIVAR 1000 ASTL, based on a PE-UHMW grade with extremely high molecular weight, has been specifically developed for tough anti-abrasion applications. TIVAR 1000 ASTL shows a higher wear and abrasion.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® ECO PE-UHMW reprocessed (ISO Data) This grade, partially composed of reprocessed PE-UHMW material, has an overall lower property level than the virgin TIVAR 1000 and a lower cost. Compared with virgin PE 500, however, it has a much b.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | Partial Break; ISO 179-1/1eA |
Quadrant EPP TIVAR® SuperPlus PE-UHMW + specific additives (ISO Data) TIVAR SuperPlus is a wear optimised, partially cross-linked PE-UHMW material with extremely high degree of polymerisation for use in most demanding applications and environments. When used for drain.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179 |
Manifattura Cattaneo PE UMW Polyethylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | |
Aardvark Polymers Aardalloy® 3300 POM Alloy Rotational Molding Resin Aardalloy 3300 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3300 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Charpy Impact, Notched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Grupo Repol Dinalon® A1X25 HI PA66 High Impact Mechanical properties for Dry As Molded samplesInformation provided by Grupo Repol |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® C 230 PA6, Conditioned Description: Unreinforced polyamide PA6, with improved impact resistance, for injection molding.Available in: EuropeProduct Applications: This grade has improved impact strength and higher flexibili.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® V2105U PBT Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO Data |
Styron CALIBRE™ 200 10 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO Data |
Styron CALIBRE™ 2060 10 Polycarbonate, Sterilization Grade CALIBRE® 2060 series resins are designed for those applications which use steam or ethylene oxide for sterilization. This material has excellent retention of physical properties and optical clari.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO Data |
Styron CALIBRE™ 300 10 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO Data |
Styron CALIBRE™ MEGARAD 2080 10 Polycarbonate, Gamma Radiation Resistant CALIBRE® MegaRad 2080 series resins provide end-users of radiation sterilized medical devices a color closer to the water-clear look of the natural resin. When exposed to high energy radiation (g.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® V2105U PBT (Europe-Africa-Middle East) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Charpy Impact, Notched | >= 9.00 J/cm² | >= 42.8 ft-lb/in² | Requirement |
Westlake Plastics Lennite® GUR1050 (Type II) Ultra-high Molecular Weight Polyethylene For Medical Applications Medical grade Lennite UHMWPE is produced from premium resins in accordance with ASTM specification F648 and International Standard ISO 5834-1 for surgical implants. Westlake Plastics' proprietary m.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179-1 |
Unitika ET2025 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® AZ 3 PA66 Product description: Grilon AZ 3 is a normal viscosity, high impact modified PA66 injection molding grade. Grilon AZ 3 has the following important properties: Excellent toughness at low temperatures.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® AZ 3/2 PA66 Product description: Grilon AZ 3/2 is an unreinforced and impact modified PA66 injection molding grade. Grilon AZ 3/2 has the following important properties: Excellent toughness at low temperaturesE.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4071 black 9992 PA612 Product description: Grilamid XE 4071 BLACK 9992 is an impact modified unreinforced high viscosity polyamide 612 (PA612) extrusion grade with superior heat and hydrolysis resistance. Compared to sta.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4071 nat PA612-I Product description: Grilamid XE 4071 NATURAL is an unreinforced impact modified high viscosity polyamide 612 (PA612) extrusion grade with superior hydrolysis and heat resistance. Compared to standa.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4188 black 9992 PA612 Product description: Grilamid XE 4188 black 9992 is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 black 9992 are: High v.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4188 nat PA612 Product description: Grilamid XE 4188 natural is a high viscosity, unreinforced, impact resistant polyamide 612 (PA612) extrusion grade. Unique features of Grilamid XE 4188 natural are: High viscosi.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 100STE NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 100STE NC010 (formerly DE20590) is a high-viscosity super-toughened acetal homopolymer with very low VOC emissions. P.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® V2105U PBT (Asia Pacific) Unreinforced, Wear resistant, UV Stabilized PBT designed for outdoor, agricultural, industrial and automotive applications. This grade has very high impact strength to stiffness ratio. |
|||
Charpy Impact, Notched | 9.00 J/cm² | 42.8 ft-lb/in² | Partial Break |
Eastman Eastalloy DA107 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |