Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® SC164 NC010 PBT
(Unverified Data**) Crastin® SC164 NC010 is an unreinforced, low viscosity polybutylene terephthalate resin for injection molding. It has been developed for consideration into applications such as parts for the health.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Shell Carilon® D26FX100 Polyketone, General-Purpose Extrusion Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26FX100 is a general-purpose extrusion grade with mechanical properties that classify it as an eng.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa EDISTIR PD RK5512G High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,088-06-07-23 UL94 V-2, polybromobiphenylether (PBBE) free, high impact polystyrene with good mechanical and thermal pr.. |
|||
Charpy Impact, Notched | 0.400 - 1.20 J/cm² | 1.90 - 5.71 ft-lb/in² | Average value: 0.842 J/cm² Grade Count:12 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Charpy Impact, Notched | 0.400 - 2.10 J/cm² | 1.90 - 9.99 ft-lb/in² | Average value: 1.28 J/cm² Grade Count:12 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Charpy Impact, Notched | 0.400 - 1.30 J/cm² | 1.90 - 6.19 ft-lb/in² | Average value: 0.700 J/cm² Grade Count:3 |
Overview of materials for Nylon 6, Glass Fiber/Solid Lube Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber/Solid Lube Filled". Each property range of values reported is minimum and maximum v.. |
|||
Charpy Impact, Notched | 0.400 - 1.50 J/cm² | 1.90 - 7.14 ft-lb/in² | Average value: 0.981 J/cm² Grade Count:24 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | |
LATI Laticonther 75 CPG/650 PBT, Glass Fiber Reinforced High thermal conductivity product based on Polybutylene Terephthalate (PBT). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | |
LATI Latilub 66-01M G/15 PA66, 15% Glass Fiber Reinforced, Molybdenum disulphide Filled Self-lubricating product based on Polyamide 66 (PA66). Molybdenum disulphide. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem 1000FV PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact Compliant, NSF 51 Listing.This data wa.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics ULTEM HU1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179-1 |
Unitika A3030N-2 PA6, 30% Mineral Reinforced, Dry Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 |
Total PPH 9082 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9082 is a controlled-rheology and antistatic homopolymer. PPH 9081 is characterized by a narrow molecular weight distribution and excellent flow properties, providing impr.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 |
Total PPH 9089 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9089 is a very low molecular weight distribution homopolymer propylene, with anti gas-fading stabilization. ApplicationATOFINA Polypropylene PPH 9089 is intended for the ex.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | IS0179-1:2000 |
Zhejiang Juner JEPP263 Weatherability PP Series Applications: Air Conditioning SystemInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® L 20 LF grey PA12 Product Description: Grilamid L 20 LF grey is a medium viscosity graphite filled Polyamide 12 (PA12) grade suitable for both injection molding and extrusion applications. Grilamid L 20 LF grey has b.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TSM-30/4 PA666-MD30 Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Crastin® SC164 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for the Healthcare Industry Crastin SC164 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection moldin.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® FG400XRD NC010 Acetal (POM)
(Unverified Data**) X-ray Detectable Medium Viscosity Acetal Copolymer Developed for Food Contact Applications Delrin FG400XRD NC010 is a filled medium viscosity acetal copolymer for injection molding. It is detected i.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 2600 PC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | ISO 179 |
BASF Ultramid® 8231G HS BK-102 14% Glass Filled PA6 (Dry) Ultramid 8231G HS BK-102 is a black pigmented heat stabilized, 14% glass fiber reinforced PA6 injection molding compound.The glass fiber reinforcement enhances performance such as strength, stiffnes.. |
|||
Charpy Impact, Notched | 0.400 - 1.50 J/cm² | 1.90 - 7.14 ft-lb/in² | Average value: 1.07 J/cm² Grade Count:11 |
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TS V0 X PA666 FR Product description: Grilon XE 5030 is a heat stabilized, flame retardant and self-extinguishing injection molding grade on the basis of PA6-PA66-alloy. Grilon XE 5030 features the following main pr.. |
|||
Charpy Impact, Notched | 0.400 J/cm² | 1.90 ft-lb/in² | |
BASF Novolen® 1104 K Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.400 - 0.650 J/cm² | 1.90 - 3.09 ft-lb/in² | Average value: 0.575 J/cm² Grade Count:4 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |