Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Asia Pacific) Extem XH2315 Resin |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Europe-Africa-Middle East) Extem XH2315 Resin |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RV330 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | |
Ineos ABS Lustran® 1460, Injection Grade
(discontinued **) Injection molding grade, increased heat and impact resistance, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acqui.. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | |
Polimeri Europa SINKRAL PD G523 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-25-20 High impact injection moulding grade. Other characteristics: good flow, excellent thermal stabilit.. |
|||
Charpy Impact, Notched | 2.40 - 10.0 J/cm² | 11.4 - 47.6 ft-lb/in² | Average value: 4.60 J/cm² Grade Count:4 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | |
Ineos ABS Lustran® 248 Key Features:UnfilledSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO 179 |
Menzolit Menzolit® BMC 1500 Unsaturated Polyester UP BMC 1500 is a special BMC for the use at elevated temperature. The glass content is set to a level that combines good flowability with good strength and stiffness properties. Even without a specific.. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | |
Ineos ABS Lustran® H701 Medium heat resistance, high impact strength. ,Property data per ISO test methods. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | |
Styrolution NOVODUR® P2MC ABS, Injection Grade Injection molding grade for plating; very good ratio between toughness, heat resistance and flow.Applications: All parts to plating: e.g. sanitary parts. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO Data |
Styron Magnum™ 2620 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO Data |
Styron Magnum™ 2645 ABS, Impact Grade MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO Data |
Styron Magnum™ 541 ABS, High Impact MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO Data, Low Temp |
Styron Pulse® 840P ABS + Polycarbonate PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin.. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO Data, Low Temp |
Styron Pulse® EXT 100 ABS + Polycarbonate PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering .. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO 179-1 |
Vyncolit Neopreg Kinel® SK4503 S5 Aramid Reinforced Molding Compound Long aramid fiber reinforced BMI molding compound suited for very demanding tribologic applications under medium to poor lubricated conditions, high temperatures & PV levelsInformation provided by S.. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW241F10 (COND) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) 25% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G25HS BK117 is a 25% glass fiber reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information p.. |
|||
Charpy Impact, Notched | 2.40 J/cm² @Temperature 23.0 °C |
11.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Charpy Impact, Notched | 2.40 J/cm² | 11.4 ft-lb/in² | ISO Data |
Styron Magnum™ 9020 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM AB.. |