Mechanical Properties Metric English Comments
Charpy Impact, Notched 0.420 J/cm²

@Temperature -40.0 °C
2.00 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 HH-TFGV 1530 Nylon 6.6 for injection molding, 15% PTFE lubricated, 30% glass fiber reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.420 J/cm²
2.00 ft-lb/in²
ISO 179/1eA
Radici Raditer® BN100 Polybutylene Terephthalate
PBT General PurposeInformation provided by Radici group.
Charpy Impact, Notched 0.420 J/cm²

@Temperature 23.0 °C
2.00 ft-lb/in²

@Temperature 73.4 °F
Injection Molded; ISO 179/1eA
PolyOne Bergadur™ PB400 G10 H UF UV Polybutylene Terephthalate (PBT)
Information provided by PolyOne
Charpy Impact, Notched 0.420 J/cm²

@Temperature -40.0 °C
2.00 ft-lb/in²

@Temperature -40.0 °F
DIN 53453
Nilit FRIANYL A63 HH-SG-GV 2020 Nylon 6.6 for injection molding, 20% mineral filled, 20% glass fiber reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Charpy Impact, Notched 0.420 J/cm²

@Temperature 23.0 °C
2.00 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c..
Charpy Impact, Notched 0.420 - 1000 J/cm²
2.00 - 4760 ft-lb/in²
Average value: 0.770 J/cm² Grade Count:5
Overview of materials for Nylon 11, Cable Sheathing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o..
Charpy Impact, Notched 0.420 - 1.06 J/cm²

@Temperature -30.0 - -30.0 °C
2.00 - 5.04 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.712 J/cm² Grade Count:5
Overview of materials for Nylon 11, Cable Sheathing Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o..
Charpy Impact, Notched 0.420 - 0.460 J/cm²

@Temperature -30.0 - -30.0 °C
2.00 - 2.19 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 0.440 J/cm² Grade Count:2
Overview of materials for Nylon 11 with Graphite Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with Graphite Filler". Each property range of values reported is minimum and maximum values of ..
Charpy Impact, Notched 0.420 - 0.560 J/cm²
2.00 - 2.67 ft-lb/in²
Average value: 0.490 J/cm² Grade Count:6
Overview of materials for Nylon 12, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap..
Charpy Impact, Notched 0.420 J/cm²
2.00 ft-lb/in²
ISO 179/1eA
Lucite International Diakon® TD642 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Charpy Impact, Notched 0.420 J/cm²
2.00 ft-lb/in²
ISO 179/1eA
Polyplastics Duranex® HN7315 Polybutylene Terephthalate (PBT), Low warpage, 15% GF filled
DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers ..
Charpy Impact, Notched 0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
Eastman Eastar 6763 PETG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Charpy Impact, Notched 0.420 J/cm²

@Temperature 23.0 °C
2.00 ft-lb/in²

@Temperature 73.4 °F
EN ISO 179
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Charpy Impact, Notched 0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Conditioned)
Designation ISO 1874-PA12,EHLS,22-010,CD10Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Very low friction coefficient. No..
Charpy Impact, Notched 0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® AMN G8 TLD Nylon 12, Graphite Filled (Conditioned)
Designation ISO 1874-PA12,MHLS,14-010,CD05Rigid grade with graphite filler for injection molding. Available colors: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient..
Charpy Impact, Notched 0.420 J/cm²
2.00 ft-lb/in²
Arkema Group Rilsan® AUM 50 NOIR T6LD Nylon 12, 50% Glass Bead Filled (Dry)
Designation ISO 1874-PA12,MHLR,16-020,GB50Rigid grad with glass beads filler (50%) for injection molding. Available color: black. Reinforced light and heat stabilizing agents. Mold-release agent.Goo..
Charpy Impact, Notched 0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BESN G9 TL Nylon 11, Graphite Filled (Dry)
Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good ..
Charpy Impact, Notched 0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
Arkema Group Rilsan® BESN P40 W5 TL Nylon 11, Flexible Tubing Grade (Conditioned)
Designation ISO 1874-PA11-P,EFHL,22-003Flexible grade for tubes extrusion. Available color: milky white. Light and heat stabilized. Flame retardant agent.Fire-resistant. Flexibility. High impact str..
Charpy Impact, Notched 0.420 J/cm²
2.00 ft-lb/in²
Arkema Group Rilsan® MB 3000 Nylon 11, Sheathing Grade (Dry)
Designation ISO 1874-PA11,MF,12-010Polyvalent rigid grade for injection molding and sheathing of cables. Available color: natural. Flame retardant agent, halogen free. Fire-resistant. Easy to be pro..
Charpy Impact, Notched 0.420 J/cm²

@Thickness 2.00 mm,
Temperature 20.0 °C
2.00 ft-lb/in²

@Thickness 0.0787 in,
Temperature 68.0 °F
ASTM D256
Mitsui TPX® MX002 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Charpy Impact, Notched 0.420 J/cm²

@Thickness 2.00 mm,
Temperature 20.0 °C
2.00 ft-lb/in²

@Thickness 0.0787 in,
Temperature 68.0 °F
ASTM D256
Mitsui TPX® MX004 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Charpy Impact, Notched 0.420 J/cm²

@Thickness 2.00 mm,
Temperature 20.0 °C
2.00 ft-lb/in²

@Thickness 0.0787 in,
Temperature 68.0 °F
ASTM D256
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Charpy Impact, Notched 0.420 J/cm²

@Thickness 2.00 mm,
Temperature 20.0 °C
2.00 ft-lb/in²

@Thickness 0.0787 in,
Temperature 68.0 °F
ASTM D256
Mitsui TPX® RT18 XB Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Charpy Impact, Notched 0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.