Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Charpy Impact, Notched | 0.250 - 0.350 J/cm² @Temperature 23.0 °C |
1.19 - 1.67 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eA |
Raschig Group 3535 Epoxy Glass fiber-reinforced epoxy molding compound. Good mechanical strength, very good electrical isolation properties adn dimensional stability even at high temperatures. Form: Low dust granulate pack.. |
|||
Charpy Impact, Notched | 0.250 - 0.400 J/cm² @Temperature 23.0 °C |
1.19 - 1.90 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group 6552 DAIP Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Charpy Impact, Notched | 0.250 - 0.400 J/cm² | 1.19 - 1.90 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Charpy Impact, Notched | 0.250 - 0.350 J/cm² | 1.19 - 1.67 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group RALUPOL® 4802 UP Polyester Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u.. |
|||
Charpy Impact, Notched | 0.250 - 2.50 J/cm² @Temperature -30.0 - -20.0 °C |
1.19 - 11.9 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.841 J/cm² Grade Count:49 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Charpy Impact, Notched | 0.250 - 1.24 J/cm² @Temperature -30.0 - -30.0 °C |
1.19 - 5.90 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.640 J/cm² Grade Count:24 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 80-7580/BK Polyacetal-copolymer, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -23.0 °C |
1.19 ft-lb/in² @Temperature -9.40 °F |
DIN 53453 |
Global PP-1100-PK Polypropylene Homopolymer Description-transparency, high stiffness, high heat resistantApplications-general purpose, household goodsInformation provided by Global Polymers Corporation. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179 eA |
Lehmann & Voss LUVOCOM® 80-7919 Polyacetal-copolymer, with PTFE, easy flowing Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -20.0 °C |
1.19 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Global PP-2300-SC Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-thin walled parts, electrical appliancesInformation provided by Global Polymers Corporation. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | |
LATI Latigray 53/22-01 CX/70 PP Homopolymer, Impact Modified Radiopaque compound based on Polypropylene homopolymer (PPh), impact modified. Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformati.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Styrolution Luran® 388 S SAN Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis HH315MO Polypropylene HH315MO is a polypropylene homopolymer intended for injection molding. Its high melt flow makes it especially suitable for products with long flow length. This grade is designed for high-speed injec.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PP MONSTEN® MA 230 Polypropylene Homopolymer Applications include injection molding. Antistatic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179 |
Vyncolit X655 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent dimensional stability and a very low coefficient of thermal expansion. UL listed.USES: Automotive disc brake pistons and gask.. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ EE260AE Scratch Resistant Polypropylene Compound Daplen EE206AE is a 20% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE206AE is optimized to provide excellent scratch resistance on gained and unpai.. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179 |
Unitika TERRAMAC TE-7307 Polylactic Acid (PLA) Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addilene H 490 M20S Flame Retardant Polypropylene, 20% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 2309 L Polypropylene Cast film and thermoformed partsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 2348 M Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 2348 TC Polypropylene Grade with nucleating and antistatic agents for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179 |
BASF Ultramid® NFX-0102 NF2004 30% Glass Filled PA66 (Dry) Ultramid NFX-0102 NF2004 is a heat stabilized, 30% glass bead PA66 injection molding grade. It is especially formulated for low warp, increased stiffness and excellent dimensional stability. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature -30.0 °C |
1.19 ft-lb/in² @Temperature -22.0 °F |
|
Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Conditioned) Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good t.. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene H 442 M30 Polypropylene Homopolymer High heat resistance, detergent stabilizedInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.250 J/cm² @Temperature 23.0 °C |
1.19 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH T5060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.250 - 1.10 J/cm² @Temperature -30.0 - -30.0 °C |
1.19 - 5.24 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 0.629 J/cm² Grade Count:7 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact, Notched | 0.250 J/cm² | 1.19 ft-lb/in² | |
Arkema Group Oroglas® V 045 I Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 045 I is an extrusion that exhibits the following properties : 50% tougher than standard acrylics excellent optical properties ( comparable to that of standard acrylics) superior surface .. |