Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
Murtfeldt Murytal® C Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO2039.1 DIN.53456 |
Omnia Plastica PSU Polysulphone It is a non-reinforced amorphous polymer whose main features are its high thermal, electrical and mechanical properties which are typical of a crystalline polymer. Compared to its "brother" PES it h.. |
|||
Ball Indentation Hardness | 140 - 155 MPa | 20300 - 22500 psi | ISO.2039-2 |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Nilit FRIANYL A63 W Nylon 6.6 for injection molding Nylon 6.6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Nilit FRIANYL B63 KG20 Nylon 6 for injection molding, 20% chalk filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Quadrant EPP Ertacetal® C POM-C, extruded (ISO Data) Ertacetal C is Quadrant’s copolymer acetal grade. Next to the standard natural and black grades, there is also a series of special colours available all showing an FDA food contact compliant compos.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Quadrant EPP Ertacetal® H-TF POM-H, PTFE-filled, extruded (ISO Data) Ertacetal H-TF is a DELRIN® AF Blend, a combination of TEFLON® fibres evenly dispersed in a DELRIN acetal resin. Much of the strength that is inherent in Ertacetal H is retained. Some properties c.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Nilit FRIANYL A63 GV 5 Nylon 6.6 for injection molding, 5% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Nilit FRIANYL C73 T Nylon 6.6/6 for injection molding Nylon 6.6/6 for injection molding, medium viscosity, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 140 - 290 MPa | 20300 - 42100 psi | Average value: 237 MPa Grade Count:20 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® AS LF 20 PA66-Z20 Product description: Grilon AS LF 20 is a heat stabilized, normal viscosity PA 66 injection molding grade with 20% lubricant (PTFE + silicon oil). Grilon AS LF 20 has the following important propert.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BS/2 PA6 Product description: Grilon BS/2 is an unreinforced, nucleated standard PA6 injection molding grade with normal melt viscosity. Grilon BS/2 has the following important properties: Good flow behavior.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT3Z black 9564 PA* Product description: Grivory HT3Z is an unreinforced and impact resistant, engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT product is partially ba.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HT3Z black 9564 PA* Product description: Grivory HT3Z is an unreinforced and impact resistant, engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT product is partially ba.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® HT3Z LF black 9564 PA* Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® HT3Z LF black 9564 PA* Product description: Grivory HT3Z LF is an unreinforced and impact resistant, PTFE modified engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT produc.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSS/2 FA PA666 Product description: Grilon TSS/2 FA is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/2 FA has the following important properties: Excellent flow .. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSS/4 LF 1 PA666 Product description: Grilon TSS/4 LF 1 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 1% lubricant (molybdenum disulphide). Grilon TSS/4 LF 1 has the following import.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® BG-50 HM PA6-GF50 Product description: Grilon BG-50 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 50% glass fibers. Grilon BG-50 HM has the following important prop.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 300 POM Basic, fast cycling injection molding grade suitable for many applications.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 400 LS POM Injection molding grade based on Tarnoform 400 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 400 POM Easy flowing, fast cycling injection molding grade for manufacturing of thin-wall detailsInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
BASF Ultradur® S 4090 G2 10% Glass Filled PBT Description: Is a PBT + ASA, easy-flowing injection-molding grades with 10% glass fibers; for rigid, tough and dimensionally stable technical parts e. g. housings, consoles, contact carriers, covers.. |
|||
Ball Indentation Hardness | 140 MPa @Load 36.5 kg, Time 30.0 sec |
20300 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2770 K POM Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
CENTROPLAST CENTROGUARD Polyoxymethylene, Antimicrobial During the modification with POM CG, antimicrobial substances are included in the basic polyoxymethylene polymer, which provide an effective and long lasting solution against unwanted growth of micr.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | value at 30 sec.; ISO 2039-1 |
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer CENTRODAL C is a versatile material with good chemical resistance, good machinability, and surface slip properties. Applications include sliding components and rollers, toothed wheels, ratchets, an.. |
|||
Ball Indentation Hardness | 140 MPa | 20300 psi | ISO 2039-1 |
CENTROPLAST CENTRODAL W Polyoxymethylene POM W is a semi-crystalline thermoplastic, which is certified in accordance with the regulatory system DVGW, technical regulations, work form W 270 and therefore, is particularly suited for the safe.. |