Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D-790 |
Plaskolite Optix® CA - 41 UVT LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging JGR 136A Clear 13FG Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D-790 |
Plaskolite Optix® CP - 41 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L0152 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 80.6 MPa | 11700 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L0659 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D-790 |
Plaskolite West Optix® CP - 41 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
Network Polymers Kepital® F20-52 Description: Natural Acetal Copolymer, Weather Resistance GradeInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
PolyOne Geon™ SF M7120 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
SABIC Innovative Plastics LNP COLORCOMP D1000P PC LNP* COLORCOMP* D1000P is an unfilled Polycarbonate. Added feature of this grade is: Exceptional Processing. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PX09322 PA 6 (Asia Pacific) White colored thermally conductive mineral filled PA6 FR compound |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D-790 |
Plaskolite West Optix® CA - 41 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO Data |
Styrolution Terluran® HH-112 ABS Terluran HH-112 is an injection molding grade of ABS with very high heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Styrolution Terluran® HH-112 Q42 Gray 10072 ABS Description: Injection-molding grade with highest heat resistance, high rigidity and medium impact strength.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
Styron Pulse® 2100LG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP D7002IXH PC LNP* THERMOCOMP* D7002IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces, housings, etc., in healthcare an.. |
|||
Flexural Strength | 80.7 MPa | 11700 psi | ASTM D790 |
Chase Plastics CP Pryme® N313GL (COND, 50% RH) Nylon 6 (Utility Grade), 13% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ASTM D790 |
Plenco 2000 Phenolic, Granular, Injection Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Polyplastics Tepcon M25 Acetal-copolymer (POM), High Viscosity Information provided by PolyPlastics. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ASTM D790 |
Plenco 7476 Phenolic, Granular, Transfer Molded PLENCO 07476 is a cotton flock filled resole phenolic molding compound, with improved physical strength, crack resistance, and is resistant to soap and detergent solutions at elevated temperatures. .. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ASTM D790 |
Unitika FUN-8000 Characteristics: High impact strength High chemical resistance Transparency as high as polycarbonateInformation provided by Unitika Ltd. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Ascend Performance Materials Vydyne® 49 Nylon 66, DAM Vydyne® 49 is a general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved imp.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ASTM D790 |
A. Schulman ComAlloy Comtuf® 522 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Ascend Performance Materials Vydyne® 49 Nylon 66, Impact Modified, DAM Vydyne® 49 is general-purpose, impact-modified PA66 resin. Available in natural, is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact s.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Ascend Performance Materials Vydyne® 49H NT Nylon 66, Impact Modified, DAM Vydyne® 49H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat-stabilized for improved resista.. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Polyplastics Duracon® M25-44/M25S Acetal Co-polymer (POM), Standard, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ISO 178 |
Polyplastics Duracon® M25-45 Acetal Co-polymer (POM), Weather resistance, High viscosity DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 80.4 MPa | 11700 psi | 2.8 mm/min; ASTM D790 |
Samsung Cheil Industries Infino® TK-2046H PCT, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Flexural Strength | 81.0 MPa | 11700 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL002 PC (Asia Pacific) LNP LUBRICOMP* DL002 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |