Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 70.0 MPa | 10200 psi | STN EN ISO 178 |
Plastcom SLOVALEN PC 51 T 20 Polypropylene Copolymer, 20% Micronized Talc FeaturesModified copolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden f.. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | |
Plastcom SLOVALEN PC 53 T 25 PP, 25% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 25% microground, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitu.. |
|||
Flexural Strength | <= 70.0 MPa | <= 10200 psi | ISO 178 |
Polykemi AB POLYabs R00 ABS, High Impact Information provided by Polykemi AB |
|||
Flexural Strength | 70.3 MPa | 10200 psi | ASTM D790 |
Oxford Polymers 802-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ISO 178 |
Nilit FRIANYL B63 TF30 Nylon 6 for injection molding, 30% PTFE lubricated Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 70.0 - 110 MPa | 10200 - 16000 psi | Compression; ISO 178 |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Flexural Strength | 70.0 - 90.0 MPa | 10200 - 13100 psi | Compression; ISO 178 |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 1-7968 Polyamide 66, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Dynamic stressed parts.Isotrop.. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | |
Lehmann & Voss LUVOCOM® 1850/TF/30 PBT, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Flexural Strength | 70.3 MPa | 10200 psi | initial |
Malvern Minerals Thermoplastic Polyester with Novacite® 1250 Quartz Filler Product data demonstrates the effect of the Novacite (untreated lamellar quartz) filler. A separate entry demonstrates the effect of surface-treated Novakup filler in thermoplastic polyester Th.. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | 2mm/min; ASTM D790 |
Kingfa HR-527A Modified ABS Features:UL94 HB @ 1.5-3.2mmHeat resistanceApplications:Automobile partsAutomobile audioDashboard, interior trimAutomobile lamp, mirrorInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | 2mm/min; ASTM D790 |
Kingfa PBT-T15 15% Mineral Filled PBT Features:Excellent size stabilityLow tendency to wrapLow abrasionGood surfaceApplications:Injection moldingApplication partsE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL0049EF PC LNP* Lubricomp* DL0049EF is a compound based on Polycarbonate resin containing 20% PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Flame Retardant |
|||
Flexural Strength | 70.0 MPa | 10200 psi | DIN 54352 |
Schwartz Technical Plastics LAMIGAMID® 320 Cast Polyamide 6, Conditioned Application: heavy-duty wheelsInformation provided by Schwartz Technical Plastics GmbH |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ISO 178 |
Styrolution Novodur® 4105 ABS Novodur Ultra 4105 is a PC modified high heat injection molding grade with high impact strength.Information provided by Styrolution |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermotuf R1000EI2 PA 66 (Europe-Africa-Middle East) High Impact Nylon 66 compound containing Impact Modifier.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ISO 178 |
Styrolution Terlux® HD 2822 MABS Terlux® HD 2822 is a new standard-injection molding grade based on a MABS polymer. Terlux® HD 2822 offers a well balanced combination of stiffness and toughness and the high transparency well .. |
|||
Flexural Strength | 70.3 MPa @Thickness 3.17 mm |
10200 psi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® SR-0310 Heat Resistant Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ASTM D790 |
A. Schulman POLYFORT™ FPP 1220 Glass Filled Chemically Coupled Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1220 is a 20% glass filled chemically coupled impact copolymer polypropylene product.Information provided by A. Schulman. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ASTM-D790 |
Polyram RamShine PV507 ABS, Flame Retardant Flame retardant ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ASTM-D790 |
Polyram RamShine PAS701 ASA, UV Stabilized UV stabilized general purpose injection molding ASAInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | dry; ISO 178 |
DSM EcoPaXX® Q-E7300 PA410-I Tube Extrusion |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ISO 178 |
Eurostar Staramide R1000EI2 PA66, Impact Modified, Injection Molded Staramide R1000EI2 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | Dry; ISO 178 |
Arkema Group Orgalloy® RS 6000 Polyamide 6 Alloy Polyamide Alloy, Rigid grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, DAM Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, DAM Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 GB2 POM 10% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Flexural Strength | 70.0 MPa | 10200 psi | ISO 178 |
Polyram RamShine PAS703 ASA, UV Stabilized Is a general purpose injection molding ASA, good chemical resistance, UV stabilization.Information provided by Polyram. |