Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 97.0 MPa | 14100 psi | |
Plastcom SLOVAMID 66 LI PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | |
Plastcom SLOVAMID 66 LI TS PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
IDI Composites 44-10 MW Thermoset Polyester, Molding Moderate strength material specifically formulated for microwave oven performance.Data provided by the manufacturer. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
IDI Composites W-102 Thermoset Polyester, Molding Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
Kolon KOCETAL® K700BK Colored Grade Acetal Resin Colored, low viscosity grade.Applications: Thin products, improved appearance.Information provided by API-Kolon. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | |
Haysite 18600 Polyester BMC, 15% Glass Reinforced The 18600 series bulk molding compound can be compression, transfer, or injection molded. Formulated with a high temperature resin system, this grade exhibits exceptional retention of physical and e.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP OL004 PPS - Linear LNP* LUBRICOMP* OL004 is a compound based on PPS - Linear resin containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RL4040HSUV PA 66 LNP* LUBRICOMP* RL4040HSUV is a compound based on Nylon 66 containing 20% PTFE. Added features of this grade include: Heat Stabilized, UV Stabilized, Wear Resistant. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
Stratasys® Polycarbonate A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating strong parts .. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 201-10 Polycarbonate Resin Overview: CALIBREâ„¢ 201-10 is produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. It provides excellent impact resistance, heat distortion resi.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 201-22 Polycarbonate Resin Overview: CALIBREâ„¢ 201-22 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 301-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 301-15 Polycarbonate Resin Overview: CALIBREâ„¢ 300-115 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity. The CALIBREâ„¢ 300-10 series products are available in 4 .. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 301-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet applic.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 301EP-22 Polycarbonate Resin Overview: CALIBREâ„¢ 300EP-22 Series are polycarbonate resins that offer exceptional impact resistance, heat distortion resistance and optical clarity for injection molding applications. Their hi.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 200-23 Polycarbonate Resin Overview: CALIBREâ„¢ 200-23 polycarbonate resins are produced in compliance with the US Food and Drug Administration (FDA) and EU food contact regulations. They provide excellent impact resistanc.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2.0 mm/min; ISO 178 |
Styron CALIBREâ„¢ 300-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 polycarbonate resin offer exceptional impact resistance, heat distortion resistance, and optical clarity as high melt strength for blow molding and sheet applications. .. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 3-point; ISO 178 |
Styron CALIBREâ„¢ 302-6 Polycarbonate Resin Overview: CALIBREâ„¢ 300-6 Polycarbonate resins offer exceptional impact resistance, heat distortion resistance, and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
Lubrizol Isoplast® 2531 Engineering Thermoplastic Polyurethane Resin for Medical Applications Features: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ISO 178 |
Unitika A1030FR PA6, Dry Information provided by Unitika Ltd. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | |
Cosmic Plastics K31 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | |
Cosmic Plastics K77 Short Glass Fiber Filled Iso Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
Plenco 7500 Phenolic, Granular, Compression Molded PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
Covestro Makrolon® 2256 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
Covestro Makrolon® 2665 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medium viscosity, easy.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | 2 mm/min; ISO 178 |
Covestro Makrolon® 3158 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 221 ABS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4.. |
|||
Flexural Strength | 97.0 MPa | 14100 psi | |
Cosmic Plastics D33 Short Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |