| Category | Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced |
| Manufacturer | Kolon |
| Trade Name | Kocetal® |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Kolon KOCETAL® K700BK Colored Grade Acetal Resin.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.41 g/cc | 1.41 g/cc | ASTM D792 |
| Moisture Absorption at Equilibrium | 0.22 % | 0.22 % | 60% RH; ASTM D570 |
| Linear Mold Shrinkage | 0.020 cm/cm | 0.020 in/in | ASTM D955 |
| Melt Flow | 27 g/10 min | 27 g/10 min | ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 80 | 80 | ASTM D785 |
| Tensile Strength | 65.0 MPa | 9430 psi | ASTM D638 |
| Elongation at Break | 40 % | 40 % | ASTM D638 |
| Flexural Strength | 97.0 MPa | 14100 psi | ASTM D790 |
| Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
| Izod Impact, Notched | 0.530 J/cm | 0.993 ft-lb/in | ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 130 µm/m-°C | 72.2 µin/in-°F | ASTM D696 |
| Melting Point | 166 °C | 331 °F | ASTM D1525 |
| Deflection Temperature at 0.46 MPa (66 psi) | 159 °C | 318 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 110 °C | 230 °F | ASTM D648 |
| Vicat Softening Point | 162 °C | 324 °F | ASTM D1525 |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+14 ohm-cm | 1.00e+14 ohm-cm | ASTM D257 |
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | ASTM D257 |
| Dielectric Constant | 3.7 | 3.7 | ASTM D150 |
| Dielectric Strength | 19.0 kV/mm | 483 kV/in | ASTM D149 |
| Dissipation Factor | 0.0060 @Frequency 1.00e+6 Hz |
0.0060 @Frequency 1.00e+6 Hz |
ASTM D150 |