Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | <= 87.0 MPa | <= 12600 psi | ISO 178 |
Polykemi AB POLYasa 2410F High Flow ASA Information provided by Polykemi AB |
|||
Flexural Strength | 87.0 - 125 MPa | 12600 - 18100 psi | ASTM D790 |
Proto3000 Accura® Amethyst™ Material for use with Viper™ SLA® systems Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. FEATURES:Outstanding accuracyExceptional detailHigh thermal resistanceDeep purple colorLow as.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Nilit FRIANYL A63 HS-GV10 Nylon 6.6 for injection molding, 10% glass fiber reinforced Nylon 6.6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
PTS POM-90 Acetal Copolymer Information provided by PTS LLC. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL002F PC LNP LUBRICOMP* DL002F is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Superior Molding. |
|||
Flexural Strength | <= 87.0 MPa | <= 12600 psi | ISO 178 |
Polykemi AB POLYform POM C M20 Polyoxymethylene Information provided by Polykemi AB |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
NOVA Chemicals DYLARK® 238 Impact Grade Engineering Resin Features:High heat resistance Good chemical resistance High impact strength Excellent flow characteristicsApplications:Automotive interior trim applications Automotive consoles Structural HousingsIn.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP BX02715 SAN LNP* LUBRICOMP* BX02715 is a compound based on SAN containing proprietary fillers. Added features of this grade include: Wear Resistant, Tight Dimensional Tolerance, Good for Water Meter Applicati.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
Kolon KOCETAL® LW701 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY D20009 PC (Asia Pacific) LNP LUBRILOY* D20009 is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Flame Retardant. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66 LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DD200C PC (Asia Pacific) PTFE free polycarbonate compounds with ESD safety and good lubricating perfomrance , suitable for Semiconductor and Hard Disk Drive (HDD) and semicon industry. Added features of this material includ.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DX93500 PC LNP STAT-KON* DX93500 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP MF741XXH PP LNP* THERMOCOMP* MF741XXH is a compound based on Polypropylene reain containing Glass Fiber and proprietay antimicrobial additives. Designed for touch surfaces in patient critical healthcare applic.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp OX92080 PPS - LINEAR LNP* Thermocomp* OX92080 is a compound based on Linear PPS containing Proprietary Fillers.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RB006 PA 66 LNP* THERMOCOMP* RB006 is a compound based on Nylon 66 resin containing 30% Glass Bead. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
Plenco 2408 Phenolic, Granular, Compression Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Polyplastics Tepcon M90 Acetal-copolymer (POM), General Information provided by PolyPlastics. |
|||
Flexural Strength | 87.0 MPa @Strain 3.50 % |
12600 psi @Strain 3.50 % |
ISO 178 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Flexural Strength | 87.0 MPa @Strain 3.50 % |
12600 psi @Strain 3.50 % |
ISO 178 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM Test |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ASTM D790 |
A. Schulman ComAlloy Aqualoy® 125 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an.. |
|||
Flexural Strength | 87.0 - 125 MPa | 12600 - 18100 psi | ASTM D790 |
3D Systems Accura® Amethyst™ Plastic for Viper™ SLA® Systems Optimized for the rapid and automated production of patterns and master molds for jewelry manufacturing. For use with Viper™ SLA® systems.ApplicationsPatterns for use with low and high vulcanizing.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Polyplastics Duracon® CP-15X Acetal Co-polymer (POM), Creep resistant, Creep resistant DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Polyplastics Duracon® M90-45 Acetal Co-polymer (POM), Weather resistance, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Polyplastics Duracon® M90-71 Acetal Co-polymer (POM), Heat resistance DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Ascend Performance Materials Vydyne® 25WSP Nylon 66, Dry as Molded Vydyne® 25WSP is a black, weather-resistant injection-molding grade PA66 resin. This resin offers a well-balanced combination of engineering properties characterized by high strength, rigidity, goo.. |
|||
Flexural Strength | 87.0 MPa | 12600 psi | ISO 178 |
Polyplastics Duracon® M90-44/M90S Acetal Co-polymer (POM), Standard, General DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |