Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2320 LCW Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2710 Polyvinyl Chloride, Rigid (PVC, Rigid) This product is available in opaque and transparent colors.Information provided by PolyOne |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
PolyOne LubriOne™ PC-000/15T Polycarbonate (PC) Information provided by PolyOne |
|||
Flexural Strength | 82.7 MPa | 12000 psi | Lengthwise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NX9300 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | Lengthwise; IPC-TM-650.2.4.4 |
Park Electrochemical Nelco® NY9233 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Quadrant EPP Acetron® POM-C Copolymer Acetal, Porosity-Free, Unfilled, Extruded |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Polymer Resources PC-GP1-10TFE Polycarbonate, General Purpose, Wear Resistant, Low Flow Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Polymer Resources PPX-FR2-[color]-EN Modified-PPO, V-1 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-1 Flame Retardant, 210F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Ravago Manufacturing Americas Hybrid S451H Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Flame Retardant High Flow RoHS Compliant UL File Number: E157012 Form: Pellets Processing Method: Injection Molding Information provided by Ravago |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Polymer Resources PC/TP-GP1 PC Polyester, High Impact, Good Chemical Resistance
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Polymer Resources NY66-IM1-[color]H Nylon, Medium Impact Modified, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Quadrant EPP Duratron® PAI T4540 Polyamide-imide, compression molded (ASTM Product Data Sheet) |
|||
Flexural Strength | 82.7 MPa @Thickness 3.17 mm |
12000 psi @Thickness 0.125 in |
ASTM D790 |
PTS Tristar® PC-10R-CL02(V38) 38 MFI Polycarbonate with Release Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000TL Nylon 6/6 (DAM)
(discontinued **) Information provided by Entec. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
A. Schulman ComAlloy® E-12672 Polyester Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D-790 |
Axiall ProTherm® 4529 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4529 CPVC is a pelletized injection molding compound designed for large fittings. Typical applications are in potable water and chemical transfer systems especially where hi.. |
|||
Flexural Strength | 82.7 - 89.6 MPa | 12000 - 13000 psi | |
Bulk Molding Compounds BMC 1603 Multi-purpose grade BMC 1603 is a multi-purpose, moderate strength, low cost material that is suitable for injection, compression and transfer molding. UL® recognized. This material was formerly known as Glastic® 160.. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D-790 |
Axiall 8258 Rigid PVC, Extrusion Georgia Gulf 8258 is a special purpose rigid PVC for film and food grade sheet compound. It has been used where packages are manufactured to FDA guidelines.Information provided by Georgia GulfGeorg.. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Aclo Accucomp Polystyrene GS0500L Low Impact |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D790 |
Adell EL-18 Homopolymer Polypropylene, 40% Mineral Filled; Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 82.7 MPa | 12000 psi | ASTM D-790 |
Plaskolite West Optix® CA - 900 High Impact Acrylic Resin Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g.. |