Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Multibase Nylex™ 2112 FR V0 Natural Polyamide + PP Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Network Polymers Nylon 6615 L Description: Black Super Tough NylonInformation provided by Network Polymers Inc. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Polymer Resources PPX-FR1-[color]EN Modified PPO, UL 94 V-0 with HDT of 190 F, Extrusion Grade Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
PolyOne Lubri-Tech™ PS-15GB/10T Polybutylene Terephthalate (PBT), Glass Bead Filled, PTFE Lubricated
(discont Description/Features:Glass Bead FilledPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
PolyOne Lubri-Tech™ ATH-5KV/000 Acetal-Homopolymer, Aramid Fiber
(discontinued **) Description/Features:Aramid Fiber ReinforcedInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed black onlyInformation provided by MRC Polymers Inc. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | |
SGL Carbon Group EK 20 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Techmer ES Electrablend® HDPE 04001 LE BK Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ESD Protection and ConductiveAppearance: BlackProcessing Method: ExtrusionInformation provided by .. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6 FR IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Techmer ES HiFill® PP CO GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 55.2 MPa @Thickness 3.17 mm |
8000 psi @Thickness 0.125 in |
ASTM D790 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Teknor Apex Chemlon® 267 Nylon 6, Impact Modified Notes: Chemlon® is a product offering flexural modulus, impact and elongation properties suitable for convoluted tubing and wire coating applications. Features: Copolymer; Good Flexibility; Good .. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6 E FR Availability: North AmericaForms: PelletsFeatures: Flame Retardant Processing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D 790 |
Styrolution Clearblend 145 MBS Clearblend 145 is an impact modified styrene acrylic copolymer blend with excellent clarity.Excellent clarityLow densityEase of processingLow moisture absorptionInformation provided by Styrolution |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Chase Plastics CP Pryme® N300STL (DAM) Nylon 6 (Utility Grade), Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Chase Plastics CP Pryme® NN100STL (DAM) Nylon 66, Super Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static) Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in th.. |
|||
Flexural Strength | <= 55.2 MPa | <= 8000 psi | ASTM D790 |
Arkema Group Solarkote® PB Acrylic For PVC/acrylic alloys Information provided by Arkema Group |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Polymer Resources PPX-FR1 Modified PPO, UL 94 V-0 with HDT of 190 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
PolyOne Edgetek® UR-30GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Strength | 55.2 MPa | 8000 psi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 FR IM Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 55.2 MPa | 8010 psi | ASTM D790 |
PolyOne LubriOne™ ATH-05KV/000 Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |