Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 45.0 MPa | 6530 psi | |
Plastcom SLOVALEN PC 81 T 15 PP, 15% mineral filling FeaturesModified copolymer PP for injection moulding with the content of 15% micronized, floated, chemically modified talc. General application - packing material, garden flower-pots, toys, furnitur.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | |
Plastcom SLOVAMID 66 SHI PA66, improved strength Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PP EIP12030F Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PP HBK15030 D Polypropylene, Multifiller High Gloss, Detergent Resistant Information provided by Polykemi AB |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PP HBK15030 Polypropylene, Multifiller High Gloss Information provided by Polykemi AB |
|||
Flexural Strength | 45.0 - 60.0 MPa | 6530 - 8700 psi | ASTM D790-03 |
Proto3000 Objet Digital Materials™ DM_8505Gray50 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: TangoBlackPlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to pr.. |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PPHC K2040H Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PPHC TS25020 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PPC K6020 S Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PPH T15010 H VTUV1 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 45.0 - 47.0 MPa @Temperature 23.0 °C |
6530 - 6820 psi @Temperature 73.4 °F |
2.5 mm/min; ASTM D790 |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
Ineos Nova Styrosun® 6600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA12 (Europe-Africa-Middle East) LNP* LUBRICOMP* SP003 is a compound based on PA 12 resin containing PTFE/Silicone. Added features include: Internally Lubricated. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | |
SPS Guang Zhou SAMATâ„¢ 5000A Flame-retarded Polypropylene Characteristic: Good flame retardance, non-halogen, high flow properties, high rigidity, high heat resistance, meets the requirements of RoHs and PaHsApplications: Lighting fitting, E/E applianceInf.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ISO 178 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-LOY AX06484 ABS LNP* STAT-LOY* AX06484 is a compound based on ABS resin containing Talc. Added feature of this grade is: Antistatic, Extrudeable. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
Polyram PlusTek RD104 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
A. Schulman POLYFLAM™ RPP 1360 Non-Halogenated Homopolymer Polypropylene DescriptionPolyflam® RPP 1360 is a UL 94 V0 rated, non-halogenated homopolymer polypropylene flame retardant compound. Information provided by A. Schulman. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | 2 mm/min; ISO 178 |
Chi Mei Polyrex® PH-888G Polystyrene - High gloss High impact; high gloss |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
Entec Hypro™ PPH-T20 Homopolymer Polypropylene, 20% Talc Reinforced Information provided by Entec |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0334T20L Talc Reinforced |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ISO 178 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, Conditioned Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Flexural Strength | 45.0 MPa | 6530 psi | |
Plastcom SLOVALEN PH 73 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PPHC K1035 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 45.0 MPa | <= 6530 psi | ISO 178 |
Polykemi AB POLYfill PPHC K9030 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 45.0 MPa | 6530 psi | ISO 178 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, Conditioned Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |