Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 35.0 MPa | 5080 psi | STN EN ISO 178 |
Plastcom PLASTALEN® PH 52 T 20 003/1M Polypropylene reinforced with 20% mineral filler PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 81 N 003 Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | STN EN ISO 178 |
Plastcom SLOVALEN PH 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 130°C... |
|||
Flexural Strength | 35.0 MPa | 5080 psi | |
Plastcom SLOVALEN PH 96 FRD 1 PP, flame retardant FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | |
Plastcom SLOVALEN PQ 81 T 25 PP, 25% mineral filling FeaturesModified PP for injection moulding with the content of 25% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decreased shri nkage. Gen.. |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PP CQX10030E10 F Polypropylene, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PPC T4020 E20 Polypropylene Copolymer, Mineral Reinforced, Modified Information provided by Polykemi AB |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PPC TS6020 E20 Polypropylene Copolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Flexural Strength | 35.0 MPa | 5080 psi | |
Pyrotek NT-C Electrical Insulating Material NT-C offers superior arc and heat resistance properties, with adequate strength properties to withstand mechanical stress and hold up in severe electrical insulating applications. NT-C does not pro.. |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB SCANFILL Injection CPC15051 PP/PE, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PP EIP8020F Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | <= 35.0 MPa | <= 5080 psi | ISO 178 |
Polykemi AB POLYfill PPH B8065 VT1 Polypropylene Homopolymer, Mineral Reinforced, Heat Resistant Information provided by Polykemi AB |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Nilit FRIANYL C73 HS28 Nylon 6.6/6 for injection molding Nylon 6.6/6 for injection molding, medium viscosity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Nilit FRIANYL C73 S10 Nylon 6.6/6 for injection molding Nylon 6.6/6 for injection molding, medium viscosity, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Strength | 35.0 MPa @Temperature 23.0 °C |
5080 psi @Temperature 73.4 °F |
2mm/min; 80x10x4mm; ISO 178 |
SYNTHOS Krasten® 662E High Impact Polystyrene High impact grade with properties suitable for thermoforming. Processed mainly by extrusion and thermoforming. Production of demanding visual appearance plates, technical parts, sheets and molded pa.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP M7001XXH PP LNP* THERMOCOMP* M7001XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additves. Designed for touch surfaces in patient critical healthcare applications. Added f.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP M7002XXH PP LNP* THERMOCOMP* M7002XXH is a compound based on Polypropylene resin containing proprietary antimicrobial additives. Designed for touch surfaces in healthcare applications. Added features include:.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Polyram RamOfin PPC101 Polypropylene Copolymer, Heat Stabilized Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ASTM-D790 |
Polyram RamShine PS503 Polystyrene, Flame Retardant Flame retardant, high impact polystyrene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Ecomass® 3011ZD86 Tungsten Filled Polycarbonate Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Filled Polycarbonate (PC) CompoundGood ToughnessInformation provided by Tech.. |
|||
Flexural Strength | 35.0 MPa | 5070 psi | ASTM D790 |
CPC - Vycom SEABOARD™ Premier High density polyethylene (HDPE) Seaboard High Density Polyethylene (HDPE) is the toughest marine grade polymer sheet available. This UV stable product has scratch resistance, excellent impact, and stiffness, yet it is easy to mach.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | 2 mm/min; ISO 178 |
Chi Mei Polyrex® PH-88 Polystyrene - High Impact High impact |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336C10L Calcium Reinforced |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ASTM D790 |
Aclo Accutech Polypropylene Homopolymer HP0336C40L Calcium Reinforced |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ASTM Test |
BASF Ultramid® 8202 PA6 (Conditioned) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | |
Biomer P226 PHB Biodegradable Polymer PHB is a isotactic, absolutely linear, thermoplastic homopolyester built of 3-hydroxy butyric acid. The formula of the subunit is -[O-CH(CH3)-CH2-CO]-. PHB is free from even traces of catalysts. P.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ASTM D790 |
Teknor Apex Sinelec CCB6814 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Features: Electrically Conductive Uses: Corrugated Sheet Forms: Pellets Processing Method: Injection Method; Sheet Extr.. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
Polyram RamOfin PPC104 Polypropylene Copolymer Heat stabilized polypropylene copolymer for injection molding applications.Information provided by Polyram. |
|||
Flexural Strength | 35.0 MPa | 5080 psi | ISO 178 |
SABIC Innovative Plastics LNP Stat-kon MX01767C PP LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB.. |