Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Oxford Polymers 30GF 30% Glass Fiber Filled Polycarbonate for Injection Molding 30% Glass Fiber Filled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Flexural Strength | 159 MPa | 23100 psi | |
Pyrotek TS-106 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Tan / Red color. High heat resistance. UL recognized.Information provided by Pyrotek. |
|||
Flexural Strength | 159 MPa | 23100 psi | |
Pyrotek TS-106 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resinApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulators Exhaust duct insulators Machined parts Wedges & shunts Point feeder gasketsAdvant.. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003F PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. This product has thinwall FR capability and has a UL94 V0 listing. This material is RoHS compliant.. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Europe-Africa-Middle East) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Quadrant EPP Ketron® 1000 IM Injection Molded Unfilled Polyetheretherketone (ASTM Product Data Sheet) Excellent chemical resistance Very low moisture absorption Inherently good wear and abrasion resistance Unaffected by continuous exposure to hot water or steam |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Quadrant EPP Ketron® GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Polymer Resources PPX-MF-FRG20 Modified-PPO, 40% Glass/Mineral Reinforced, Flame Retardant Modified-Polyphenylene Oxide, 40% Glass/Mineral Reinforced, Flame RetardantFeatures: • Bromine Free • Chlorine Free • Self ExtinguishingProcess: Injection MoldingNotes: All physical, mechanica.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Polymer Resources TPSF-GP1 PBT, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1013TL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1033THL Nylon 6/6 (Cond) Information provided by Ravago. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1040MHL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Polymer Resources NY66-M40-[color]H Nylon, 40% Mineral Filled, Lubricated, Heat Stabilized (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Quadrant EPP Ketron® GF30 LSG PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone (ASTM Product Data Sheet) |
|||
Flexural Strength | 159 MPa | 23000 psi | |
XXX Phenolic Laminate Paper based phenolic provides low cost electrical and mechanical properties. It is widely used for switchboards, panel boards, insulating washers, and intricate punched parts.Information provided b.. |
|||
Flexural Strength | 159 MPa | 23100 psi | |
Haysite ETS Glass Reinforced Polyester Sheet, Electrical Grade (GPO1) A NEMA GPO-1 economy grade fiberglass mat reinforced thermoset polyester molded sheet. ETS is an IEEE Class B 130ºC electrical/160ºC mechanical material with good punching characteristics. Typ.. |
|||
Flexural Strength | 159 MPa | 23100 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON DE002 PC (Asia Pacific) LNP* Stat-Kon* DE002 is a Polycarbonate containing Carbon Fiber. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate.. |
|||
Flexural Strength | 159 MPa | 23100 psi | ASTM D790 |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
A. Schulman SCHULADUR® A GF15 15% Glass Fiber Reinforced PBT Information provided by A. Schulman. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
Ensinger HYDLAR® Z Nylon, Pultruded Aramid Fiber Reinforced (PA) HYDLAR® possesses a combination of physical properties that cannot be found in any other commercially available engineered plastic. Design engineers have created a family of superior wear and abra.. |
|||
Flexural Strength | 159 MPa | 23000 psi | |
Anderman Ceramics EM60 Mullite Synthetic mullite available in rod, tube, sheaths and insulators up to 10 ft (3 m) long with diameters 0.3" to 19".Information provided by Anderman Ceramics. |
|||
Flexural Strength | 159 MPa | 23000 psi | ASTM D790 |
PolyOne Edgetek® PI-20GM/000 L Polyetherimide (PEI), Glass Filled
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedHigh FlowPolyOne First ChoiceInformation provided by PolyOne Corporation. |