Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.55 MPa @Strain 300 % |
1240 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® F02-081A-6C TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Stress | 8.55 MPa @Strain 100 % |
1240 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3890 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 8.54 MPa @Strain 1.63 %, Temperature 90.0 °C |
1240 psi @Strain 1.63 %, Temperature 194 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.55 MPa @Strain 300 % |
1240 psi @Strain 300 % |
2.0 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1000-92 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Stress | 8.55 MPa @Strain 300 % |
1240 psi @Strain 300 % |
2.0 in/min; ASTM D412 |
Teknor Apex Telcar® TL-1000-92-UV Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tensile Stress | 8.55 MPa @Strain 0.250 %, Temperature 40.0 °C |
1240 psi @Strain 0.250 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 8.52 MPa @Strain 0.200 %, Temperature -40.0 °C |
1240 psi @Strain 0.200 %, Temperature -40.0 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 8.53 MPa @Strain 0.500 %, Temperature 80.0 °C |
1240 psi @Strain 0.500 %, Temperature 176 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 8.52 MPa @Strain 100.56 %, Temperature 100 °C |
1240 psi @Strain 100.56 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.52 MPa @Strain 24.0 %, Temperature 90.0 °C |
1240 psi @Strain 24.0 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.56 MPa @Strain 37.24 %, Temperature 90.0 °C |
1240 psi @Strain 37.24 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.52 MPa @Strain 100.56 %, Temperature 100 °C |
1240 psi @Strain 100.56 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.52 MPa @Strain 24.0 %, Temperature 90.0 °C |
1240 psi @Strain 24.0 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.56 MPa @Strain 37.24 %, Temperature 90.0 °C |
1240 psi @Strain 37.24 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.53 MPa @Strain 150.01 %, Temperature 120 °C |
1240 psi @Strain 150.01 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.53 MPa @Strain 50.9 %, Temperature 90.0 °C |
1240 psi @Strain 50.9 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.52 MPa @Strain 0.400 %, Temperature 60.0 °C |
1240 psi @Strain 0.400 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D.. |
|||
Tensile Stress | 8.57 MPa @Strain 0.700 %, Temperature 80.0 °C |
1240 psi @Strain 0.700 %, Temperature 176 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D.. |
|||
Tensile Stress | 8.52 MPa @Strain 0.100 %, Temperature 40.0 °C |
1240 psi @Strain 0.100 %, Temperature 104 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA) Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p.. |
|||
Tensile Stress | 8.56 MPa @Strain 0.150 %, Temperature 90.0 °C |
1240 psi @Strain 0.150 %, Temperature 194 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 8.52 MPa @Strain 11.52 %, Temperature 150 °C |
1240 psi @Strain 11.52 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by.. |
|||
Tensile Stress | 8.55 MPa @Strain 133.56 %, Temperature 120 °C |
1240 psi @Strain 133.56 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |