Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 84.7 MPa @Strain 0.710 %, Temperature 23.0 °C |
12300 psi @Strain 0.710 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 85.0 MPa @Strain 2.50 %, Temperature 60.0 °C |
12300 psi @Strain 2.50 %, Temperature 140 °F |
|
Solvay TECHNYL® A 218 V25 Black 21 N PA66, 25% glass fiber, DRY Description: TECHNYL® A 218 V25 is a polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 85.0 MPa @Strain 3.00 %, Temperature 80.0 °C |
12300 psi @Strain 3.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 85.0 MPa @Strain 6.00 %, Temperature 120 °C |
12300 psi @Strain 6.00 %, Temperature 248 °F |
|
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, Conditioned Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The .. |
|||
Tensile Stress | 85.0 MPa @Strain 4.00 %, Temperature 100 °C |
12300 psi @Strain 4.00 %, Temperature 212 °F |
|
Solvay TECHNYL® A 218W V33 Natural T PA66, 33% glass fiber, DRY Description: TECHNYL® A 218W V33 Nat T is a polyamide 66, reinforced with 33% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The prod.. |
|||
Tensile Stress | 85.0 MPa @Strain 3.00 % |
12300 psi @Strain 3.00 % |
|
Solvay TECHNYL® A 221 PA66, DRY Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef.. |
|||
Tensile Stress | 85.0 MPa @Strain 2.00 % |
12300 psi @Strain 2.00 % |
|
Solvay TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits:.. |
|||
Tensile Stress | 85.0 MPa @Strain 4.00 %, Temperature 60.0 °C |
12300 psi @Strain 4.00 %, Temperature 140 °F |
|
Solvay TECHNYL® A 60 G1 V25 PA66, 25% glass fiber, DRY Description: TECHNYL® A 60G1 V25 is a 25% GF reinforced organophosphorous flame retarded grade based on a patented high flow polyamide 66 resin. This product is heat stabilized and provides optim.. |
|||
Tensile Stress | 85.0 MPa @Strain 3.00 % |
12300 psi @Strain 3.00 % |
|
Solvay TECHNYL® C 218 V 30 PA6, 30% glass fiber, Conditioned Description: TECHNYL® C 218 V30 is a polyamide 6, heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is available in black color.Benefits: The product offers.. |
|||
Tensile Stress | 85.0 MPa @Strain 1.00 % |
12300 psi @Strain 1.00 % |
|
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, DRY Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is.. |
|||
Tensile Stress | 85.0 MPa @Strain 1.00 % |
12300 psi @Strain 1.00 % |
|
Solvay TECHNYL® A 218W V30 Natural PA66, 30% glass fiber, DRY Description: TECHNYL® A 218W V30 Nat is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural color.Benefits: The produc.. |
|||
Tensile Stress | 84.5 MPa @Strain 18.2 %, Temperature -20.0 °C |
12300 psi @Strain 18.2 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Tensile Stress | 84.5 MPa @Strain 5.60 %, Temperature -20.0 °C |
12300 psi @Strain 5.60 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Tensile Stress | 84.5 MPa @Strain 5.60 %, Temperature -20.0 °C |
12300 psi @Strain 5.60 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Tensile Stress | 84.5 MPa @Strain 3.50 %, Temperature 23.0 °C |
12300 psi @Strain 3.50 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Tensile Stress | 84.9 MPa @Strain 0.700 %, Temperature -40.0 °C |
12300 psi @Strain 0.700 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Tensile Stress | 84.82 MPa @Strain 1.46 %, Temperature 23.0 °C |
12300 psi @Strain 1.46 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Stress | 84.81 MPa @Strain 1.25 %, Temperature 90.0 °C |
12300 psi @Strain 1.25 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |
|||
Tensile Stress | 84.8 MPa @Strain 3.10 %, Temperature 23.0 °C |
12300 psi @Strain 3.10 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 84.6 MPa @Strain 0.880 %, Temperature 40.0 °C |
12300 psi @Strain 0.880 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Stress | 85.0 MPa @Strain 4.00 %, Temperature 40.0 °C |
12300 psi @Strain 4.00 %, Temperature 104 °F |
ISO 527 |
BASF Ultradur B 4300 G4 20% Glass Filled PBT Ultradur B4300 G4 is an easy flowing injection molding PBT with 20% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
Tensile Stress | 85.0 MPa @Strain 4.00 % |
12300 psi @Strain 4.00 % |
|
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |