Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.90 MPa @Strain 300 %, Thickness 2.00 mm |
1150 psi @Strain 300 %, Thickness 0.0787 in |
Type 1, 200 mm/min Across Flow; DIN 53504 |
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE) OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi.. |
|||
Tensile Stress | 7.90 MPa @Strain 300 % |
1150 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ V 3085A-S0098 Thermoplastic Elastomer (TPE) OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolef.. |
|||
Tensile Stress | 7.93 MPa @Strain 300 % |
1150 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® F02-138A TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Stress | 7.93 MPa @Strain 100 % |
1150 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3991 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 7.93 MPa @Strain 300 % |
1150 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-97-T0207A-110 Thermoplastic Elastomer Uses: Automotive Applications; Industrial Cable Insulation Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:.. |
|||
Tensile Stress | 7.96 MPa @Strain 232.29 %, Temperature 120 °C |
1150 psi @Strain 232.29 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.90 MPa @Strain 6.00 %, Temperature 23.0 °C |
1150 psi @Strain 6.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.96 MPa @Strain 46.83 %, Temperature 100 °C |
1150 psi @Strain 46.83 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.93 MPa @Strain 3.49 %, Temperature 0.000 °C |
1150 psi @Strain 3.49 %, Temperature 32.0 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.90 MPa @Strain 6.00 %, Temperature 23.0 °C |
1150 psi @Strain 6.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.96 MPa @Strain 46.83 %, Temperature 100 °C |
1150 psi @Strain 46.83 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.93 MPa @Strain 65.39 %, Temperature 100 °C |
1150 psi @Strain 65.39 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.91 MPa @Strain 0.330 %, Temperature 90.0 °C |
1150 psi @Strain 0.330 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 79G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Toughened Polyamide 66 Zytel 79G13L NC010 is a 13% glass fiber reinforced toughened polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.92 MPa @Strain 0.400 %, Temperature 150 °C |
1150 psi @Strain 0.400 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G15HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 15% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G15HSLR NC010 is a 15% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |
|||
Tensile Stress | 7.91 MPa @Strain 0.180 %, Temperature 120 °C |
1150 psi @Strain 0.180 %, Temperature 248 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 7.94 MPa @Strain 0.110 %, Temperature 150 °C |
1150 psi @Strain 0.110 %, Temperature 302 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |
|||
Tensile Stress | 7.90 MPa @Strain 6.00 %, Temperature 40.0 °C |
1150 psi @Strain 6.00 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 7.94 MPa @Strain 100.62 %, Temperature 120 °C |
1150 psi @Strain 100.62 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 7.91 MPa @Strain 48.45 %, Temperature 120 °C |
1150 psi @Strain 48.45 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 7.90 MPa @Strain 10.0 %, Temperature 23.0 °C |
1150 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8136BK TPC-ET
(Unverified Data**) Hytrel® HTR8136BK is designed for blow molding or processing by techniques requiring high melt viscosity. It has nominal durometer hardness of 49D, is pigmented black with fine particle size carbon.. |
|||
Tensile Stress | 7.96 MPa @Strain 8.44 %, Temperature 60.0 °C |
1150 psi @Strain 8.44 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.91 MPa @Strain 48.45 %, Temperature 120 °C |
1150 psi @Strain 48.45 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |