Polymer Property : Izod Impact, Notched = 5.60 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.99 J/cm

@Thickness 3.17 mm
5.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
PTS Trilac® ABS-HH2000 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 2.99 J/cm

@Thickness 3.17 mm
5.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
PTS Trilac® ABS-HS5500 High Impact ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 2.99 J/cm

@Thickness 3.17 mm
5.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
PTS Trilac® ABS-HF5500 High Flow ABS Resin
Information provided by Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 2.99 J/cm

@Thickness 3.17 mm
5.60 ft-lb/in

@Thickness 0.125 in
ASTM D256
Global ABS-HI-121 High Impact ABS
Information provided by Global Polymers Corporation.
Izod Impact, Notched 2.99 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
5.60 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM-D256
Ineos ABS Lustran® 256/Lustran® 752 Blended ABS Resin
50/50 pellet blend of Lustran® 256 ABS and high-impact Lustran® 752 ABS
Izod Impact, Notched 2.99 J/cm

@Temperature 4.00 °C
5.60 ft-lb/in

@Temperature 39.2 °F
1/8'' notched bar, partial failure, (refrigerator temperature); ASTM D256
Ineos R01C-01 Polypropylene Random Copolymer
This is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding. Applications that require good see-through clarity combined with good heat resistance ..
Izod Impact, Notched 2.99 J/cm

@Temperature -40.0 °C
5.60 ft-lb/in

@Temperature -40.0 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® 1101 PBT+PC (Asia Pacific)
Unreinforced, opaque polycarbonate/polyester alloy. Excellent low temperature impact plus chemical resistance to automotive fluid.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 2.99 J/cm

@Temperature -40.0 °C
5.60 ft-lb/in

@Temperature -40.0 °F
ASTM D 256
SABIC Innovative Plastics Xenoy® 5220 PBT+PC (Asia Pacific)
Unreinforced, polycarbonate-based polymer blend, excellent chemical resistance and impact.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Notched 2.99 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
5.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® ABS NAT
Availability: North AmericaForms: PelletsFeatures: General PurposeAppearance: Natural ColorInformation provided by TP Composites, Inc.
Izod Impact, Notched 2.99 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
5.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 92RK
Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Izod Impact, Notched 2.99 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
5.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® ABS LE BK
Availability: North AmericaForms: PelletsFeatures: Low ExtractablesAppearance: BlackInformation provided by TP Composites, Inc.
Izod Impact, Notched 2.99 J/cm

@Thickness 3.17 mm
5.60 ft-lb/in

@Thickness 0.125 in
TPI Porene® ABS-GA800 High Impact ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 2.99 J/cm

@Thickness 3.17 mm
5.60 ft-lb/in

@Thickness 0.125 in
TPI Porene® ABS-GA850 High Impact ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 2.99 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
5.60 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8008
Availability: North AmericaForms: PelletsFeatures: General Purpose Appearance: Natural ColorInformation provided by TP Composites, Inc.