| Category | Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded |
| Manufacturer | Global Polymers Corporation |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Global ABS-HI-121 High Impact ABS.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
| Melt Flow | 14 g/10 min <br>@Load 10.0 kg,<br> Temperature 220 °C |
14 g/10 min <br>@Load 22.0 lb,<br> Temperature 428 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 46.90 MPa <br>@Thickness 3.17 mm |
6802 psi <br>@Thickness 0.125 in |
ASTM D638 |
| Flexural Yield Strength | 73.098 MPa <br>@Thickness 3.17 mm |
10602 psi <br>@Thickness 0.125 in |
ASTM D790 |
| Flexural Modulus | 2.25 GPa <br>@Thickness 3.17 mm |
326 ksi <br>@Thickness 0.125 in |
ASTM D790 |
| Izod Impact, Notched | 2.56 J/cm <br>@Thickness 6.40 mm |
4.80 ft-lb/in <br>@Thickness 0.252 in |
ASTM D256 |
| 2.99 J/cm <br>@Thickness 3.17 mm |
5.60 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 87.8 °C | 190 °F | ASTM D648 |